BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Conditioned)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, 20% Glass Fiber Filled
Material Notes:
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire test up to 960 °C.
Information provided by BASF
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Bulk Density
0.500
-
0.800
g/cc
0.0181
-
0.0289
lb/in³
Density
1.31
g/cc
0.0473
lb/in³
ISO 1183
Moisture Absorption at Equilibrium
2.0 - 2.4 %
2.0 - 2.4 %
23°C; 50% RH; ISO 62
Linear Mold Shrinkage
0.0060
cm/cm
0.0060
in/in
Linear Mold Shrinkage, Flow
0.0080
cm/cm
0.0080
in/in
ISO 2577
Linear Mold Shrinkage, Transverse
0.0080
cm/cm
0.0080
in/in
ISO 2577
Melt Flow
157.2
g/10 min
@Load 5.00 kg,
Temperature 275 °C
157.2
g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
50.0
MPa
7250
psi
50 mm/min; ISO 527-1/-2
Elongation at Yield
6.0 %
6.0 %
50 mm/min; ISO 527-1/-2
Modulus of Elasticity
3.00
GPa
435
ksi
ISO 527-1/-2
Charpy Impact Unnotched
11.0
J/cm²
@Temperature 23.0 °C
52.3
ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+11
ohm-cm
1.00e+11
ohm-cm
IEC 60093
Surface Resistance
1.00e+10
ohm
1.00e+10
ohm
IEC 60093
Comparative Tracking Index
600
V
600
V
Test solution A; IEC 60112
Hot Wire Ignition, HWI
2.0
sec
@Thickness >=1.50 mm
2.0
sec
@Thickness >=0.0591 in
ASTM D3874-88
High Amp Arc Ignition, HAI
0.00
arcs
@Thickness >=0.700 mm
0.00
arcs
@Thickness >=0.0276 in
UL 746C
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
>=
90.0
µm/m-°C
>=
50.0
µin/in-°F
Melting Point
220
°C
428
°F
ISO 3146
Decomposition Temperature
>=
300
°C
>=
572
°F
UL RTI, Electrical
140
°C
@Thickness 1.50 mm
284
°F
@Thickness 0.0591 in
UL 746B
Oxygen Index
29 %
29 %
ISO 4589-2
Glow Wire Flammability Index
960
°C
@Thickness 1.00 mm
1760
°F
@Thickness 0.0394 in
IEC 60695-2-12
Ignition Temperature
>=
350
°C
>=
662
°F
ASTM D1929
Processing Properties
Metric
English
Comments
Processing Temperature
80.0
°C
176
°F
Hopper Throat
Zone 1
250
°C
482
°F
Feed Zone
Zone 2
260
°C
500
°F
Compression
Zone 3
270
°C
518
°F
Metering-zone
Zone 4
270
°C
518
°F
Nozzle
Melt Temperature
250
-
275
°C
482
-
527
°F
Injection-molding/Extrusion
270
°C
518
°F
Optimal
Mold Temperature
80.0
°C
176
°F
Optimal
80.0
-
90.0
°C
176
-
194
°F
Injection-molding
Drying Temperature
80.0
°C
176
°F
Dry Time
4
hour
4
hour
Moisture Content
0.030 - 0.060 %
0.030 - 0.060 %
Optimal
<= 0.15 %
<= 0.15 %
Descriptive Properties
Color
Grey 22975
Commercial Status
Europe
Peripheral Screw Speed
< 0.3 m/s
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
A. Schulman SCHULAMID® 66 GF20H 20% Glass Fiber Reinforced, Heat Stabilized Nylon 66
BASF Ultramid® B3UG4 BK 23215 20% Glass Filled PA66 FR (Conditioned)
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Dry)
BASF Ultramid® B3UG4 LS BK 23215 20% Glass Filled PA66 FR (Conditioned)
BASF Ultramid® B3UG4 LS Grey 22985 20% Glass Filled PA66 FR (Conditioned)
PBASG0325 / 131958
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.