MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Westlake Plastics Dielux® PTFE filled Acetal Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, PTFE Filled

Material Notes: Dielux PTFE filled acetal copolymer is an outstanding bearing and wear material for use in both wet and dry environments. It is frequently used in place of traditional metal and plastic bearing materials when low friction, excellent wear properties, and good dimensional stability are required. The PTFE filler allows Dielux to be used without additional lubricants in applications where grease and oil are undesirable.

Information provided by Westlake Plastics.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³ASTM D792
Water Absorption 0.20 %0.20 %ASTM D570; 24 hrs.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 44.8 MPa6500 psiASTM D638
Elongation at Break 10 - 14 %10 - 14 %ASTM D638
Flexural Yield Strength 68.9 MPa10000 psiASTM D790
Flexural Modulus 2.07 GPa300 ksiASTM D790
Izod Impact, Notched 0.427 J/cm0.800 ft-lb/inASTM D256
Coefficient of Friction, Dynamic 0.0700.070Dry vs. Steel
Coefficient of Friction, Static 0.150.15Dry vs. Steel
Limiting Pressure Velocity 0.438 MPa-m/sec12500 psi-ft/min100 fpm vs. Steel
 
Thermal PropertiesMetricEnglishComments
CTE, linear 97.2 µm/m-°C
@Temperature 20.0 °C
54.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 98.9 °C210 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient LubriOne™ ATH-000/04S Acetal (POM) Homopolymer
LATI Latilub 73/13-20T POM, PTFE Filled
LG Chemical LUCEL FW-710F Friction and Wear Resistant POM, PTEE filled
Ensinger Tecaform™ HPV 13 Acetal Homopolymer - Extruded Products (POM)
LG Chemical LUCEL FW-7005 Friction and Wear Resistant POM, Oil filled

PWEST008 / 72712

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.