System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
LATI Latilub 73/13-20T POM, PTFE Filled
Categories:
Polymer
;
Thermoplastic
;
Acetal (Polyoxymethylene, POM)
;
Acetal Copolymer, PTFE Filled
Material Notes:
Self-lubricating product based on Polyoxymethylene (POM). PTFE.
Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America
Information provided by Lati Industria Termoplastici S.p.A.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.50
g/cc
0.0542
lb/in³
Linear Mold Shrinkage, Flow
0.0215
-
0.025
cm/cm
0.0215
-
0.025
in/in
Linear Mold Shrinkage, Transverse
0.022
-
0.0245
cm/cm
0.022
-
0.0245
in/in
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
50.0
MPa
7250
psi
Elongation at Break
16 %
16 %
Elongation at Yield
5.0 %
5.0 %
Tensile Modulus
2.70
GPa
392
ksi
Charpy Impact Unnotched
4.50
J/cm²
21.4
ft-lb/in²
Charpy Impact, Notched
0.450
J/cm²
2.14
ft-lb/in²
Coefficient of Friction, Dynamic
0.090
0.090
Coefficient of Friction, Static
0.15
0.15
K (wear) Factor
2.20
x 10
-8
mm³/N-M
1.09
x 10
-10
in³-min/ft-lb-hr
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
145
°C
293
°F
Deflection Temperature at 1.8 MPa (264 psi)
90.0
°C
194
°F
Vicat Softening Point
135
°C
@Load 5.00 kg
275
°F
@Load 11.0 lb
Flammability, UL94
HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
Processing Properties
Metric
English
Comments
Melt Temperature
175
-
200
°C
347
-
392
°F
Mold Temperature
70.0
-
90.0
°C
158
-
194
°F
Drying Temperature
80.0
-
90.0
°C
@Time 10800 sec
176
-
194
°F
@Time 3.00 hour
Descriptive Properties
ISO Shrinkage - Pressure
60 MPa
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Avient LubriOne™ ATH-000/04S Acetal (POM) Homopolymer
LG Chemical LUCEL FW-710F Friction and Wear Resistant POM, PTEE filled
Ensinger Tecaform™ HPV 13 Acetal Homopolymer - Extruded Products (POM)
LG Chemical LUCEL FW-7005 Friction and Wear Resistant POM, Oil filled
LG Chemical LUCEL FW-715C Friction and Wear Resistant POM, Polymeric Wear Additive, CaCo3 Filled, Low Warpage, Antistatic
PLATH9886 / 177582
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.