MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Clariant Renol PA111G50 Nylon 66, 50% Glass Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes:

Data provided by Clariant Masterbatches

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.56 g/cc1.56 g/ccASTM D792
Filler Content 50 %50 %ASTM D2584
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 221 MPa32000 psiASTM D638
Elongation at Yield 3.0 %3.0 %ASTM D638
Flexural Yield Strength 310 MPa45000 psiASTM D790
Flexural Modulus 15.2 GPa2200 ksiASTM D790
Izod Impact, Notched 1.33 J/cm
@Temperature 22.8 °C
2.50 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 254 °C489 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 254 °C489 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 271 - 299 °C520 - 570 °F
Mold Temperature 79.4 - 107 °C175 - 225 °F
Dry Time 2 - 4 hour
@Temperature 79.4 °C
2 - 4 hour
@Temperature 175 °F
to ensure moisture content is less than 0.2%
Injection Pressure 4.96 - 8.27 MPa720 - 1200 psiSecondary
 8.27 - 13.8 MPa1200 - 2000 psiInitial
Back Pressure 0.345 - 1.72 MPa50.0 - 250 psi
Shot Size 30 - 80 %30 - 80 %
Screw Speed 20 - 100 rpm20 - 100 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Edgetek® NN-50GF/000EM Nylon 6/6, Glass Filled
Avient Edgetek® NN-50GF/000EM L Polyamide 66 (Nylon 66)
Avient Edgetek® NN-50GF/000 Polyamide 66 (Nylon 66)
Plastcom SLOVAMID 66 GF 50 TS PA 66 reinforced with 50% glass fibre, thermal stability
A. Schulman SCHULAMID® 66 GF50H 50% Glass Fiber Reinforced, Heat Stabilized 66

PCLAR091 / 82216

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.