MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sasol Polymers PP HTV145 Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Product Description: Features: Very High flow; Narrow molecular weight distribution; Suitable for the injection molding of thing walled articles with high flow path/wall thickness ratios; Contains a nucleating agent which ensures rapid crystallization, resulting in an improved impact to stiffness balance as well as shorter cooling times; Suitable for use in extrusion coating processes where the grade offers melt curtain stability and less necking. Applications: Injection molding: Food containers; Caps and closures; Pharmaceutical containers; Thin walled packaging. Extrusion: Extrusion coating of woven PP cloth
Availability: Africa & Middle East; Asia Pacific, Europe, Latin America, North America
Additive: Mold Release; Nucleating Agent; Unspecified Additive
Features: Good Mold Release; High Flow; Homopolymer; Narrow Molecular Weight Distribution; Nucleated
Uses: Caps; Closures; Containers; Food Containers; Thin-walled Packaging; Wovens Coatings
Forms: Pellet
Processing Method: Extrusion Coating; Injection Molding

Information provided by Sasol Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.012 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.012 in/inISO 294-4
Melt Flow 50 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 10900 psiHB; ISO 2039-1
Tensile Strength, Yield 5080 psiISO 527-2/1A/50
Elongation at Break >= 50 %ISO 527-2/1A/50
Elongation at Yield 8.5 %ISO 527-2/1A/50
Tensile Modulus 239000 psiISO 527-2/1A/50
Flexural Modulus 232000 psiISO 178
Charpy Impact, Notched 1.20 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 325 °CISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 194 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 131 °FUnannealed; ISO 75-2/A
Vicat Softening Point 198 °FISO 306/B120
 311 °FISO 306/A120
 
Processing PropertiesOriginal ValueComments
Processing Temperature 104 - 140 °FHopper, Injection
 104 - 140 °FHopper, Extrusion
Rear Barrel Temperature 356 - 500 °FInjection
Middle Barrel Temperature 428 - 536 °FInjection
Front Barrel Temperature 464 - 536 °FInjection
Nozzle Temperature 428 - 536 °FInjection
Zone 1 428 - 572 °FExtrusion
Zone 2 500 - 572 °FExtrusion
Zone 3 500 - 572 °FExtrusion
Zone 4 240 - 280 °FInjection
 500 - 572 °FExtrusion
Zone 5 500 - 572 °FExtrusion
Die Temperature 500 - 572 °FExtrusion
Melt Temperature 428 - 536 °FInjection
 464 - 572 °FExtrusion
Mold Temperature 68.0 - 140 °FInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSASOL007 / 268336

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.