MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sasol Polymers PP HTV145 Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Product Description: Features: Very High flow; Narrow molecular weight distribution; Suitable for the injection molding of thing walled articles with high flow path/wall thickness ratios; Contains a nucleating agent which ensures rapid crystallization, resulting in an improved impact to stiffness balance as well as shorter cooling times; Suitable for use in extrusion coating processes where the grade offers melt curtain stability and less necking. Applications: Injection molding: Food containers; Caps and closures; Pharmaceutical containers; Thin walled packaging. Extrusion: Extrusion coating of woven PP cloth
Availability: Africa & Middle East; Asia Pacific, Europe, Latin America, North America
Additive: Mold Release; Nucleating Agent; Unspecified Additive
Features: Good Mold Release; High Flow; Homopolymer; Narrow Molecular Weight Distribution; Nucleated
Uses: Caps; Closures; Containers; Food Containers; Thin-walled Packaging; Wovens Coatings
Forms: Pellet
Processing Method: Extrusion Coating; Injection Molding

Information provided by Sasol Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.012 cm/cm0.012 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.012 cm/cm0.012 in/inISO 294-4
Melt Flow 50 g/10 min
@Load 2.16 kg,
Temperature 230 °C
50 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 75.2 MPa10900 psiHB; ISO 2039-1
Tensile Strength, Yield 35.0 MPa5080 psiISO 527-2/1A/50
Elongation at Break >= 50 %>= 50 %ISO 527-2/1A/50
Elongation at Yield 8.5 %8.5 %ISO 527-2/1A/50
Tensile Modulus 1.65 GPa239 ksiISO 527-2/1A/50
Flexural Modulus 1.60 GPa232 ksiISO 178
Charpy Impact, Notched 0.252 J/cm²1.20 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 325 °C617 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °FUnannealed; ISO 75-2/A
Vicat Softening Point 92.2 °C198 °FISO 306/B120
 155 °C311 °FISO 306/A120
 
Processing PropertiesMetricEnglishComments
Processing Temperature 40.0 - 60.0 °C104 - 140 °FHopper, Injection
 40.0 - 60.0 °C104 - 140 °FHopper, Extrusion
Rear Barrel Temperature 180 - 260 °C356 - 500 °FInjection
Middle Barrel Temperature 220 - 280 °C428 - 536 °FInjection
Front Barrel Temperature 240 - 280 °C464 - 536 °FInjection
Nozzle Temperature 220 - 280 °C428 - 536 °FInjection
Zone 1 220 - 300 °C428 - 572 °FExtrusion
Zone 2 260 - 300 °C500 - 572 °FExtrusion
Zone 3 260 - 300 °C500 - 572 °FExtrusion
Zone 4 116 - 138 °C240 - 280 °FInjection
 260 - 300 °C500 - 572 °FExtrusion
Zone 5 260 - 300 °C500 - 572 °FExtrusion
Die Temperature 260 - 300 °C500 - 572 °FExtrusion
Melt Temperature 220 - 280 °C428 - 536 °FInjection
 240 - 300 °C464 - 572 °FExtrusion
Mold Temperature 20.0 - 60.0 °C68.0 - 140 °FInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSASOL007 / 268336

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.