MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mueller Alloy 3533 Dezincification Brass (UNS C35330)
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Dezincification resistant brass suitable for high speed machining applications

Applications: The alloy is best suitable where potential corrosion (such as dezincification) may occur. Applications for this alloy include plumber's hardware, valve spindles and fittings.

Information Provided by Mueller Industries Inc.

Key Words: AS 1567, UNS C35330, BS 2873 - C2119
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.50 g/ccBased on UNS number
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 60
Tensile Strength at Break 54000 psi
Tensile Strength, Yield 24000 psi
Elongation at Break 30 %
Machinability 100 %UNS C36000 = 100%
 
Component Elements PropertiesOriginal ValueComments
Arsenic, As 0.020 - 0.25 %
Copper, Cu 59.5 - 64 %
Lead, Pb 1.5 - 3.5 %
Zinc, Zn 32.25 - 39 %Remainder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mueller Alloy 4850 Naval Brass - High Leaded (UNS C48500)
Antimonial Naval brass, UNS C46600
Phosphorized Admiralty Copper, UNS C44400, Cold Drawn and Annealed
Chemours TeflonĀ® PTFE 7A Granular Molding Powder
High Leaded naval brass, UNS C48500

NMUEL907 / 97695

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.