MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Celanese FORTRON MT9320C0 PPS, Medical Technology
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Fortron MT9320C0 is an unfilled grade used for extrusion applications. It demonstrates excellent chemical resistance and thermal stability as well as a high melt strength. Components made of this grade may be used for medical, dental, pharmaceutical, and certain food handling applications. Fortron MT9320C0 is in compliance with ISO 10993, USP Class VI and it is included in the Fortron Drug and Device Master Files at the FDA. This grade complies with the FDA Food Contact Notification (FCN-No. 40) for repeat-use applications.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ISO 1183
Water Absorption at Saturation 0.020 %0.020 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 85.0 MPa12300 psi5mm/min; ISO 527-2/1A
Elongation at Break 6.0 %6.0 %5mm/min; ISO 527-2/1A
Flexural Strength 140 MPa20300 psiISO 178
Flexural Modulus 4.20 GPa609 ksiISO 178
Izod Impact, Notched (ISO) 3.50 kJ/m²1.67 ft-lb/in²ISO 180/1A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Dielectric Constant 2.8
@Frequency 1e+6 Hz
2.8
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
Melting Point 280 °C536 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 115 °C239 °FISO 75-1, -2
Deflection Temperature at 8.0 MPa 95.0 °C203 °FISO 75-1, -2
Glass Transition Temp, Tg 90.0 °C194 °FISO 11357-1,-2,-3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 140 - 160 °C284 - 320 °Fcavity
 310 - 320 °C590 - 608 °Fhot runner
Feed Temperature 60.0 - 80.0 °C140 - 176 °F
Zone 1 290 - 300 °C554 - 572 °F
Zone 2 300 - 310 °C572 - 590 °F
Zone 3 310 - 320 °C590 - 608 °F
Zone 4 310 - 320 °C590 - 608 °F
Die Temperature 300 - 310 °C572 - 590 °F
Melt Temperature 310 - 320 °C590 - 608 °F
Drying Temperature 110 - 120 °C230 - 248 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Moisture Content <= 0.020 %<= 0.020 %
Injection Pressure 40.0 - 80.0 MPa5800 - 11600 psi
Hold Pressure 30.0 - 60.0 MPa4350 - 8700 psi
Back Pressure <= 3.00 MPa<= 435 psi
Screw Speed  50 rpm
@Diameter 55.0 mm
50 rpm
@Diameter 2.17 in
 75 rpm
@Diameter 40.0 mm
75 rpm
@Diameter 1.57 in
 120 rpm
@Diameter 25.0 mm
120 rpm
@Diameter 0.984 in
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Descriptive Properties
Injection moldingYes
Injection speedfast
Sheet extrusionYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese FORTRON® 9320C0 Polyphenylene Sulfide (PPS)
Celanese FORTRON® 9205C4 Polyphenylene Sulfide (PPS)
Quadrant Symalit® 1000 PVDF unfilled, extruded (ISO Data)
Celanese FORTRON ICE 714A PPS, 65% Mineral / Glass Reinforced
Celanese FORTRON 1140L0 PPS, 40% Glass Reinforced

PHCQ302 / 178757

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.