MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Celanese FORTRON MT9320C0 PPS, Medical Technology
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Fortron MT9320C0 is an unfilled grade used for extrusion applications. It demonstrates excellent chemical resistance and thermal stability as well as a high melt strength. Components made of this grade may be used for medical, dental, pharmaceutical, and certain food handling applications. Fortron MT9320C0 is in compliance with ISO 10993, USP Class VI and it is included in the Fortron Drug and Device Master Files at the FDA. This grade complies with the FDA Food Contact Notification (FCN-No. 40) for repeat-use applications.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccISO 1183
Water Absorption at Saturation 0.020 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 85.0 MPa5mm/min; ISO 527-2/1A
Elongation at Break 6.0 %5mm/min; ISO 527-2/1A
Flexural Strength 140 MPaISO 178
Flexural Modulus 4200 MPaISO 178
Izod Impact, Notched (ISO) 3.50 kJ/m²ISO 180/1A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Dielectric Constant 2.8
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
Melting Point 280 °C10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 115 °CISO 75-1, -2
Deflection Temperature at 8.0 MPa 95.0 °CISO 75-1, -2
Glass Transition Temp, Tg 90.0 °CISO 11357-1,-2,-3
 
Processing PropertiesOriginal ValueComments
Processing Temperature 140 - 160 °Ccavity
 310 - 320 °Chot runner
Feed Temperature 60.0 - 80.0 °C
Zone 1 290 - 300 °C
Zone 2 300 - 310 °C
Zone 3 310 - 320 °C
Zone 4 310 - 320 °C
Die Temperature 300 - 310 °C
Melt Temperature 310 - 320 °C
Drying Temperature 110 - 120 °C
Dry Time 3.00 - 4.00 hour
Moisture Content <= 0.020 %
Injection Pressure 40.0 - 80.0 MPa
Hold Pressure 30.0 - 60.0 MPa
Back Pressure <= 3.00 MPa
Screw Speed 50 rpm
@Diameter 55.0 mm
 75 rpm
@Diameter 40.0 mm
 120 rpm
@Diameter 25.0 mm
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
Injection moldingYes
Injection speedfast
Sheet extrusionYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese FORTRON® 9320C0 Polyphenylene Sulfide (PPS)
Celanese FORTRON® 9205C4 Polyphenylene Sulfide (PPS)
Mitsubishi Chemical Advanced Materials Symalit® 1000 PVDF unfilled, extruded (ISO Data)
Celanese FORTRON ICE 714A PPS, 65% Mineral / Glass Reinforced
Celanese FORTRON 1140L0 PPS, 40% Glass Reinforced

PHCQ302 / 178757

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.