MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sipchem PBT-R1-E0-020
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Product description: Sipchem PBT-R1-E0-020 is a Polybutylene Terephthalate resin, manufactured by Sipchem Chemical Company in The Kingdom of Saudi Arabia using an Inventa-Fischer Technology. PBT-R1-E0-020 is a medium viscosity neat PBT resin

Applications: Compounding

Information provided by Sahara International Petrochemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.31 g/ccASTM D1505
Viscosity Number 1.1 dl/gIntrinsic; ASTM D2857
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ASTM D1238
 
Chemical PropertiesOriginal ValueComments
Carboxyl End Groups <= 30 meq/kgISO 2114
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 57.9 MPaASTM D638
Elongation at Yield 3.6 %ASTM D638
Flexural Strength 81.8 MPaASTM D790
Flexural Modulus 2180 MPaASTM D790
Flexural Strain at Yield 8.4 %at Flexural Strength; ASTM D790
Izod Impact, Notched 27.1 J/mASTM D256
Izod Impact, Unnotched NBASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 223 °CASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 50.5 °CASTM D648
Vicat Softening Point 173.4 °CASTM D1525
Flammability, UL94 HBIEC 60695
 
Descriptive Properties
Color<3(b*), ASTM D6290

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIPCH027 / 285340

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.