MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Sika SikaBond® Universal One part advanced polyurethane, elastomeric, adhesive
Categories: Polymer; Adhesive

Material Notes: SikaBond Universal is a multi-purpose adhesive used for bonding porous and nonporous substrates, i.e. metal, glass, concrete, etc.

Where to Use: As an elastic adhesive for bonding:

  • Wood
  • Bath fixtures
  • Glass
  • Drywall
  • Concrete
  • Paver caps
  • Metal
  • Tiles
  • Stone
  • Gutters
  • Marble
  • Mirrors
  • Brick
  • Countertops, and more!

    Advantages:

    • Excellent adhesion
    • Superior green grab
    • Fast cure rate.
    • Utilizes elastic bonding technology for long term durability
    • Good weathering and water resistance.
    • Non-corrosive.
    • Can be painted over with water, oil, and rubber-based paints. (Preliminary tests recommended).
    • Water immersible after cure
    • Good weathering and water resistance

    Information provided by Sika Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatile Organic Compounds (VOC) Content 48.3 g/l48.3 g/l
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 70.0 °C158 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 4.44 - 37.8 °C40.0 - 100 °FApplication Temperature
Cure Time 120 min2.00 hourdepending on climate
 7200 - 11500 min120 - 192 hourfinal cure
Shelf Life 12.0 Month
@Temperature 4.00 - 35.0 °C
12.0 Month
@Temperature 39.2 - 95.0 °F
in original unopened cartridge
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Synthos DL 455 SB Latex
Sika Sikaflex® Crack Flex Sealant High performance, textured, self-leveling, 1-part polyurethane sealant for sealing cracks.
Chesterton ARC PW Potable Water Coating

PSIKA919 / 209826

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.