MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chesterton ARC PW Potable Water Coating  (discontinued **)
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: ARC PW is a 100% solids lining certified for NSF/ANSI 61 potable water, cold water service. It is recommended to be applied by brush, roll or spray at 500-750 microns (20-30 mils) total dry film thickness in a two coat system for valves, fittings and pumps. ARC PW has low permeability, high tensile adhesion strength, and excellent resistance to water treatment chemicals and erosive flow condition thereby making it an ideal selection for use in potable water treatment and distribution service conditions.

Benefits:

  • 100% solids, Low VOC’s
  • High voltage spark testable per NACE RP0188
  • Amine blush free formulation
  • Convenient 2:1 mix ratio
  • Extended pot life
  • Certified to NSF/ANSI 61

Suggested Uses:

  • Valves and Fittings
  • Transfer Pumps
  • Raw Water Pumps

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.59 g/cc0.0574 lb/in³Cured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8787ASTM D2240
Elongation at Break 3.15 %3.15 %ASTM D638
Flexural Strength 65.63 MPa9519 psiASTM D790
Flexural Modulus 3.72 GPa540 ksiASTM D790
Compressive Strength 70.19 MPa10180 psiASTM D695
Adhesive Bond Strength >= 2.76 MPa>= 400 psiDry Concrete; ASTM D4541
 46.83 MPa6792 psiMetal; ASTM D4541
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 23.0 °C73.4 °FWet Service (NSF 61)
 52.0 °C126 °FWet Service (General)
 62.0 °C144 °FDry Service (General)
 
Processing PropertiesMetricEnglishComments
Cure Time  720 min
@Temperature 32.0 °C
12.0 hour
@Temperature 89.6 °F
Light Load
 1080 min
@Temperature 25.0 °C
18.0 hour
@Temperature 77.0 °F
Light Load
 1440 min
@Temperature 16.0 °C
24.0 hour
@Temperature 60.8 °F
Light Load
 1440 min
@Temperature 32.0 °C
24.0 hour
@Temperature 89.6 °F
Overcoat End
 1560 min
@Temperature 32.0 °C
26.0 hour
@Temperature 89.6 °F
Full Load
 1800 min
@Temperature 25.0 °C
30.0 hour
@Temperature 77.0 °F
Overcoat End
 2160 min
@Temperature 10.0 °C
36.0 hour
@Temperature 50.0 °F
Light Load
 2160 min
@Temperature 16.0 °C
36.0 hour
@Temperature 60.8 °F
Overcoat End
 2160 min
@Temperature 25.0 °C
36.0 hour
@Temperature 77.0 °F
Full Load
 2640 min
@Temperature 10.0 °C
44.0 hour
@Temperature 50.0 °F
Overcoat End
 2880 min
@Temperature 16.0 °C
48.0 hour
@Temperature 60.8 °F
Full Load
 4320 min
@Temperature 10.0 °C
72.0 hour
@Temperature 50.0 °F
Full Load
 7200 min
@Temperature 32.0 °C
120 hour
@Temperature 89.6 °F
Full Chemical
 10100 min
@Temperature 25.0 °C
168 hour
@Temperature 77.0 °F
Full Chemical
 12600 min
@Temperature 16.0 °C
210 hour
@Temperature 60.8 °F
Full Chemical
 14400 min
@Temperature 10.0 °C
240 hour
@Temperature 50.0 °F
Full Chemical
Tack-Free Time  270 min
@Temperature 32.0 °C
4.50 hour
@Temperature 89.6 °F
 360 min
@Temperature 25.0 °C
6.00 hour
@Temperature 77.0 °F
 420 min
@Temperature 16.0 °C
7.00 hour
@Temperature 60.8 °F
 480 min
@Temperature 10.0 °C
8.00 hour
@Temperature 50.0 °F
 
Descriptive Properties
ColorBlue
 Off White

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Haynes 188 alloy, cold rolled and 1175°C solution annealed sheet
Sika SikaBond® Universal One part advanced polyurethane, elastomeric, adhesive

PPTCHS042 / 138154

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.