MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Special Metals INCONEL® alloy MA758 Ni-Cr Superalloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: INCONEL® alloy MA 758 is an oxide-dispersion-strengthened (ODS) nickel-chromium superalloy, made by mechanical alloying. It is a development of the well-established aerospace superalloy, INCONEL alloy MA 754, with its chromium content increased to 30%, to improve its performance in corrosive environments at high temperatures. The alloy's high-temperature strength is enhanced by the use of yttrium oxide for dispersion strengthening.

It is used in a range of applications including furnace skid rails, hearth rollers, jigs, tools, and other fabrications for supporting workpieces through heat-treatment processes.

It has been specified for a fueld atomizer application in diesel engines.

Information Provided by Special Metals Corporation

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.14 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 173 MPa
@Temperature 1000 °C
Bar
 180 MPa
@Temperature 1093 °C
Plate; Longitudinal
 190 MPa
@Temperature 1093 °C
Plate; Transverse
 240 MPa
@Temperature 982 °C
Plate; Longitudinal
 250 MPa
@Temperature 982 °C
Plate; Transverse
 546 MPa
@Temperature 700 °C
Bar
 853 MPa
@Temperature 200 °C
Bar
 949 MPa
@Temperature 20.0 °C
Bar
 960 MPa
@Temperature 20.0 °C
Plate; Transverse
 1030 MPa
@Temperature 20.0 °C
Plate; Longitudinal
Tensile Strength, Yield 151 MPa
@Strain 0.2 %,
Temperature 1000 °C
Bar
 160 MPa
@Strain 0.2 %,
Temperature 1093 °C
Transverse
 170 MPa
@Strain 0.2 %,
Temperature 1093 °C
Longitudinal
 220 MPa
@Strain 0.2 %,
Temperature 982 °C
Longitudinal
 220 MPa
@Strain 0.2 %,
Temperature 982 °C
Transverse
 371 MPa
@Strain 0.2 %,
Temperature 700 °C
Bar
 495 MPa
@Strain 0.2 %,
Temperature 200 °C
Bar
 560 MPa
@Strain 0.2 %,
Temperature 20.0 °C
Bar
 680 MPa
@Strain 0.2 %,
Temperature 20.0 °C
Longitudinal
 690 MPa
@Strain 0.2 %,
Temperature 20.0 °C
Transverse
Elongation at Break 4.0 %
@Temperature 1093 °C
Plate; Longitudinal
 4.0 %
@Temperature 982 °C
Plate; Longitudinal
 5.0 %
@Temperature 1093 °C
Plate; Transverse
 6.0 %
@Temperature 982 °C
Plate; Transverse
 14 %
@Temperature 20.0 °C
Plate; Longitudinal
 22 %
@Temperature 20.0 °C
Plate; Transverse
 22 %
@Temperature 200 °C
Bar
 27 %
@Temperature 20.0 °C
Bar
 29 %
@Temperature 700 °C
Bar
 29 %
@Temperature 1000 °C
Bar
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 684.1 ohm-cir-mil/ft
@Temperature 22.0 °C
 692 ohm-cir-mil/ft
@Temperature 93.0 °C
 723.5 ohm-cir-mil/ft
@Temperature 538 °C
 724.2 ohm-cir-mil/ft
@Temperature 982 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.47 µm/m-°C
@Temperature 200 °C
 13.39 µm/m-°C
@Temperature 600 °C
 14.24 µm/m-°C
@Temperature 1000 °C
 15.03 µm/m-°C
@Temperature 1400 °C
Melting Point 1375 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.30 %
Carbon, C 0.050 %
Chromium, Cr 30 %
Iron, Fe 1.0 %
Nickel, Ni 67.55 %Remainder
Titanium, Ti 0.50 %
Y2O3 0.60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Alloy Wire International RW 80 Ni-Cr Resistance Wire
Goodfellow Nichrome®, Tophet A® Nickel 80 Chromium 20 Alloy
Special Metals INCONEL® MA758 Oxide-Dispersion-Strengthened Ni-Cr Superalloy
Special Metals INCONEL® Alloy MA 754
Special Metals UDIMET® alloy R41 Ni-Cr Alloy

NINDA03 / 98894

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.