MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Special Metals INCONEL® MA758 Oxide-Dispersion-Strengthened Ni-Cr Superalloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Data provided by the manufacturer, Special Metals.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.14 g/cc0.294 lb/in³
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0001139 ohm-cm0.0001139 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.47 µm/m-°C
@Temperature 25.0 - 92.0 °C
6.928 µin/in-°F
@Temperature 77.0 - 198 °F
Mean
 13.18 µm/m-°C
@Temperature 25.0 - 316 °C
7.322 µin/in-°F
@Temperature 77.0 - 601 °F
Mean
 14.11 µm/m-°C
@Temperature 25.0 - 482 °C
7.839 µin/in-°F
@Temperature 77.0 - 900 °F
Mean
 15.03 µm/m-°C
@Temperature 25.0 - 760 °C
8.350 µin/in-°F
@Temperature 77.0 - 1400 °F
Mean
Melting Point >= 1375 °C>= 2507 °F
Solidus 1375 °C2507 °F
Maximum Service Temperature, Air 1260 °C2300 °Ffor demanding high temp uses
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.30 %<= 0.30 %
Carbon, C 0.050 %0.050 %
Chromium, Cr 30 %30 %
Iron, Fe 1.0 %1.0 %
Nickel, Ni 67.5 %67.5 %As remainder
Titanium, Ti 0.50 %0.50 %
Y2O3 0.60 %0.60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alloy Wire International RW 80 Ni-Cr Resistance Wire
Special Metals INCONEL® Alloy X-750
Special Metals UDIMET® alloy R41 Ni-Cr Alloy
Goodfellow Nichrome®, Tophet A® Nickel 80 Chromium 20 Alloy
Special Metals INCONEL® alloy MA758 Ni-Cr Superalloy

NINCO60 / 17493

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.