MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese GUR® 4152 PE-UHMW, Unfilled
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: GUR 4152 UHMW-PE is a linear polyolefin resin in powder form with a molecular weight of approximately 7.7 MM g/mol calculated using Margolies' equation. The extremely high molecular weight of this resin yields several unique properties including superior abrasion resistance and impact strength. This and GUR 4150 resins have the best abrasion resistance of all standard grades. Outstanding properties include a low coefficient of friction that results in self-lubricating, non-stick surfaces after processing. The resin is normally processed by compression molding or ram extrusion.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccISO 1183
Density of Compound 0.930 g/ccIndicative (PE only); ISO 1872-1
Moisture Absorption <= 0.0100 %23°C/50%RH; ISO 62
Viscosity Test 2800 cm³/gISO 307, 1157, 1628
 2800 cm³/gintrinsic; ISO 1628-3
 3400 cm³/gISO 1628-3
Melt Flow <= 0.10 g/10 minASTM D1238
 0.10 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 61ASTM D2240
 6115 sec; ISO 868
Ball Indentation Hardness 35.0 MPaISO 2039-1
Tensile Strength at Break 35.0 MPa50mm/min; ISO 527-2/1A
 5076 psiASTM D638
Tensile Strength, Yield 17.0 MPa50mm/min; ISO 527-2/1A
 3100 psiASTM D638
Elongation at Break 300 %
 >= 300 %ASTM D638
Elongation at Yield 20 %50mm/min; ISO 527-2/1A
 <= 20 %ASTM D638
Tensile Modulus 680 MPa50mm/min; ISO 527-2/1A
 100000 psiASTM D638
Izod Impact, Notched NBASTM D256
Charpy Impact, Notched 130 kJ/m²ISO 11542-2
Coefficient of Friction, Dynamic 0.10
Tensile Creep Modulus, 1 hour 430 MPaISO 899-1
Tensile Creep Modulus, 1000 hours 220 MPaISO 899-1
K Factor (Wear Factor) 80sand slurry method (GUR 4120=100)
Abrasion 80
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmIEC 60093
Surface Resistance >= 1.00e+12 ohmIEC 60093
Dielectric Constant 2.1
@Frequency 100 Hz
IEC 60250
 3.0
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 45.0 kV/mmIEC 60243-1
Dissipation Factor 0.00040
@Frequency 100 Hz
IEC 60250
 0.0010
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 200 µm/m-°CISO 11359-2
Specific Heat Capacity 0.440 BTU/lb-°F
 1.84 J/g-°C
Thermal Conductivity 0.410 W/m-K
Deflection Temperature at 0.46 MPa (66 psi) 65.0 °CISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °CISO 75-1, -2
Vicat Softening Point 80.0 °CISO 306
 176 °FASTM D1525
Flammability, UL94 HB
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 210 °CISO 293
 
Descriptive Properties
Mold cooling rate, K/min, ISO 29315
Other extrusionYes
PowderYes
Transfer moldingYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese GUR® 4170 PE-UHMW, Unfilled
Celanese GUR® 4150 PE-UHMW, Unfilled
Mitsubishi Chemical Advanced Materials TIVAR™ 1000 Virgin UHMW-PE, (Natural & Colors except Black)
Garland Manufacturing GAR-DUR® Ultra High Molecular Weight Polyethylene (UHMW-PE)
Celanese GUR® 4130 PE-UHMW, Unfilled

PHCQ308 / 178763

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.