MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil EVA 5008 Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: ExxonMobil™ EVA 5008 resin is a copolymer of ethylene and vinyl acetate.

Availability: Africa & Middle East, Asia Pacific, Europe, Latin America, North America and South America

Additive: Antiblock: No; Slip: 150 ppm; Thermal Stabilizer: Yes

Applications: Stretch Hood

Information provided by ExxonMobil

Key Words: Nexxstar™ EVA-00111
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.928 g/cc0.0335 lb/in³ASTM D1505
Vinyl Acetate Content 7.5 %7.5 %ExxonMobil Method
Melt Flow 0.500 g/10 min
@Load 0.00000220 kg,
Temperature 190 °C
0.500 g/10 min
@Load 0.00000475 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance 66.7 N15.0 lb (f)
Film Tensile Strength at Yield, MD 9.80 MPa1420 psiASTM D882
Film Tensile Strength at Yield, TD 6.50 MPa943 psiASTM D882
Film Elongation at Break, MD 200 %200 %ASTM D882
Film Elongation at Break, TD 620 %620 %ASTM D882
Puncture Energy 33.9 J25.0 ft-lb
Elmendorf Tear Strength MD 190 g190 gASTM D1922
Elmendorf Tear Strength TD 60.0 g60.0 gASTM D1922
Dart Drop Test 360 g0.794 lbASTM D1709A
Film Tensile Strength at Break, MD 34.0 MPa4930 psiASTM D882
Film Tensile Strength at Break, TD 29.0 MPa4210 psiASTM D882
1% Secant Modulus, MD 110 MPa16000 psiASTM D882
1% Secant Modulus, TD 131 MPa19000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 100 °C212 °FPeak
Vicat Softening Point 80.0 °C176 °F
 
Optical PropertiesMetricEnglishComments
Haze 9.40 %9.40 %ASTM D1003
Gloss 52.0 %52.0 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem VA2019A EVA Foam Copolymer
Eurofoam Evacell EVA 50/S EVA + NR Foam
Arkema OREVAC® 18211 Maleic Anhydride Grafted EVA Copolymer
Eurofoam Evacell EVA 200 EVA + PE Foam
Eurofoam Evacell XM 2001 EVA + PE Foam

PEX99294 / 175530

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.