MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 546S01 Low Viscosity UV Curable Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: TRA-BOND 546S01 is a low viscosity UV curable adhesive with a secondary heat curing system to achieve a high Tg. It exhibits excellent adhesion to glass and many other substrates, making it ideal for a wide variety of optical applications. The 546S01 also has low cure shrinkage to minimize stress. An additional post heat cure at 100-130°C is required to achieve ultimate properties.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/ccCured
Viscosity 1000 cPMixed (cp #40, 10 rpm)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 87
 
Thermal PropertiesOriginal ValueComments
CTE, linear 68.0 µm/m-°C
@Temperature 20.0 °C
Glass Transition Temp, Tg 88.0 °CUltimate Tg; TMA
Shrinkage 0.30 %Linear, UV only
 1.3 %Linear, UV plus heat
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 - 30.0 sec350-380nm
 
Descriptive Properties
Color Transparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® 305 Spectrally Transparent Epoxy
Tra-Con Tra-Bond F114 Optically Clear, Low Viscosity Blush-Free Epoxy Adhesive
Tra-Con Tra-Bond 2129 Clear Low Viscosity Epoxy Adhesive
NextGen Adhesives G907-25 Optical Epoxy Adhesive
Master Bond MB297 Ethyl Cyanoacrylate Adhesive System

PTRAC132 / 71060

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.