MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Bond 2129 Clear Low Viscosity Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 2129 is a low viscosity epoxy adhesive recommended for industrial and electronic production, repair, small casting, coating, tooling, and rigid laminating applications where a clear system with good mechanical and electrical properties is required. This easy-to-use epoxy adhesive cures at room temperature and develops strong, low shrinkage bonds to most materials - metals, ceramics and ceramic inserts, glass and glass fabrics, wood and many rigid plastics. Fully cured TRA-BOND 2129 is an effective electrical insulator with good low temperature mechanical and impact resistance properties, and outstanding resistance to water, most petroleum products, salt solutions, mild acids and alkalis and many other organic and inorganic compounds.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccMixed
Solids Content 100 %100 %Reactive Solids Content
Viscosity 1900 cP
@Temperature 25.0 °C
1900 cP
@Temperature 77.0 °F
After mixing
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8888
Adhesive Bond Strength 6.89 MPa1000 psiLap shear, alum to alum
Izod Impact, Notched 0.256 J/cm0.480 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.90e+13 ohm-cm5.90e+13 ohm-cm
 9.50e+9 ohm-cm
@Temperature 100 °C
9.50e+9 ohm-cm
@Temperature 212 °F
Dielectric Constant 4.0
@Frequency 1000 Hz
4.0
@Frequency 1000 Hz
Dielectric Strength 16.1 kV/mm410 kV/in
Dissipation Factor 0.020
@Frequency 1000 Hz
0.020
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 58.0 µm/m-°C
@Temperature 20.0 °C
32.2 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 140 °C284 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Glass Transition Temp, Tg 95.0 °C203 °FUltimate Tg
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Cure Time  240 min
@Temperature 65.0 °C
4.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 30 min30 min
 
Descriptive Properties
Color Clear, Transparent
Mix Ratio, parts by weight100/25Resin/Hardener
Thixotropic Index 1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® 305 Spectrally Transparent Epoxy
Tra-Con Tra-Bond F114 Optically Clear, Low Viscosity Blush-Free Epoxy Adhesive
Tra-Con Tra-Bond 546S01 Low Viscosity UV Curable Adhesive
NextGen Adhesives G907-25 Optical Epoxy Adhesive
Master Bond MB297 Ethyl Cyanoacrylate Adhesive System

PTRAC024 / 70952

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.