MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lanxess Addovate® RM PU Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Dispersant for the production of polyester based flexible slabstock foam

Addovate RM is used in combination with Addovate WM and Addovate SM for the production of polyester based flexible slabstock foam. When Addovate RM is used, its emulsifying effect is such that the amount of Addovate WM can be reduced by about 50% of the amount of Addovate RM used. Due allowance should be made for the water content when formulating. Addovate RM has a greater effect on the crosslinking reaction than does Addovate SM. This offers particular advantages in the production of foams with densities lower than 35 kg/m³. The amount of Addovate SM can be kept low; this has a favorable effect on the tendency to core discoloration. Scorching can also be reduced by the additional use of Addovate LM. Any consequent tendency to cracking can be offset by increasing the amount of Addovate RM -rather than increasing the proportion of Addovate SM. Too much Addovate RM leads to foams having a more closed-cell structure, or to shrinkage. The amount of Addovate RM to be used depends on the required foam density. The lower the density, the more Addovate RM must be used.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³
Viscosity 415 - 615 cP415 - 615 cP
 
Thermal PropertiesMetricEnglishComments
Boiling Point 101 °C214 °FInitial
Pour Point -17.8 °C0.000 °F
Flash Point >= 100 °C>= 212 °FASTM D92, DIN ISO 2592
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature 15.0 - 30.0 °C
6.00 Month
@Temperature 59.0 - 86.0 °F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 49 - 51 %49 - 51 %
 
Descriptive Properties
Amine number28-38 mgHCl/g
Appearancebright to yellowish, slightly turbid liquid
Hydroxyl value28

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8227 / 208620

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.