MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Escorene™ UL 05540EH2 Ethylene Vinyl Acetate Copolymer (European Grade)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product Description: UL 05540EH2 is a copolymer of ethylene and vinyl acetate.

Availability: Africa & Middle East, Asia Pacific and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
  • Free Flowing Agent: Yes
Applications:
  • Compounding
  • Hot Melt Adhesives
  • Ink Modifier
  • Wire and Cable Compounds

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.967 g/ccExxonMobil method
Vinyl Acetate Content 39 %ExxonMobil method
Melt Flow 60 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 43Molded Properties; ASTM D2240
Tensile Strength at Break >= 260 psi(20 in/min), Molded Properties; ASTM D638
Elongation at Break >= 750 %(20 in/min), Molded Properties; ASTM D638
Tensile Modulus 440 psi(0.2 in/min), Molded Properties; ASTM D638
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 118 °FPeak Melting Point; ExxonMobil method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema EVATANE® 40-55 Copolymer Ethylene - Vinyl Acetate
Dow Elvax® 40W Ethylene-Vinyl Acetate Copolymer Resin
Arkema EVATANE® 42-60 Copolymer Ethylene - Vinyl Acetate
ExxonMobil Escorene® MV-02528 EVA Copolymer, Adhesive and Sealant Grade
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade

PEX99116 / 175352

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.