System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
ExxonMobil Escorene® MV-02528 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Ethylene Vinyl Acetate
;
Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Material Notes:
Data provided by the manufacturer, Exxon Chemical.
A 27.5% vinyl acetate copolymer
Applications:
Hot melt adhesives; Wax blends; Industrial sealants.
Key Words:
Ethylene Vinyl Acetate; Exxon Chemical Company
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.937
g/cc
0.0339
lb/in³
Exxon Method
Apparent Bulk Density
0.449
g/cc
0.0162
lb/in³
ASTM D1895 (B)
Viscosity
3100
cP
@Temperature 190 °C
3100
cP
@Temperature 374 °F
melt viscosity; ASTM D-3236
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
48
48
ASTM D2240
Tensile Strength, Ultimate
9.80
MPa
1420
psi
ASTM D638
Elongation at Break
100 %
100 %
ASTM D638
Flexural Modulus, 1% Secant
4.40
MPa
638
psi
ASTM D790
Thermal Properties
Metric
English
Comments
Melting Point
62.0
°C
144
°F
Exxon Method
Ring & Ball Softening Point
76.0
°C
169
°F
ASTM E-28
Optical Properties
Metric
English
Comments
Refractive Index
1.483
1.483
Exxon Method
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Arkema EVATANE® 40-55 Copolymer Ethylene - Vinyl Acetate
ExxonMobil Escorene™ UL 05540EH2 Ethylene Vinyl Acetate Copolymer (European Grade)
Arkema EVATANE® 42-60 Copolymer Ethylene - Vinyl Acetate
Dow Elvax® 40W Ethylene-Vinyl Acetate Copolymer Resin
ExxonMobil Escorene™ MV 02514 Ethylene Vinyl Acetate Copolymer (European Grade)
PEXCEP / 37901
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.