MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Escorene® MV-02528 EVA Copolymer, Adhesive and Sealant Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade

Material Notes: Data provided by the manufacturer, Exxon Chemical.

A 27.5% vinyl acetate copolymer

Applications: Hot melt adhesives; Wax blends; Industrial sealants.

Key Words: Ethylene Vinyl Acetate; Exxon Chemical Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.937 g/ccExxon Method
Apparent Bulk Density 0.449 g/ccASTM D1895 (B)
Viscosity 3100 cP
@Temperature 190 °C
melt viscosity; ASTM D-3236
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 48ASTM D2240
Tensile Strength, Ultimate 9.80 MPaASTM D638
Elongation at Break 100 %ASTM D638
Flexural Modulus, 1% Secant 0.00440 GPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 62.0 °CExxon Method
Ring & Ball Softening Point 76.0 °CASTM E-28
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.483Exxon Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema EVATANE® 40-55 Copolymer Ethylene - Vinyl Acetate
ExxonMobil Escorene™ UL 05540EH2 Ethylene Vinyl Acetate Copolymer (European Grade)
Arkema EVATANE® 42-60 Copolymer Ethylene - Vinyl Acetate
Dow Elvax® 40W Ethylene-Vinyl Acetate Copolymer Resin
ExxonMobil Escorene™ MV 02514 Ethylene Vinyl Acetate Copolymer (European Grade)

PEXCEP / 37901

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.