MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Borealis BJ100HP Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: BJ100HP is a special low viscosity polypropylene compound developed to fit the production of PP-GF composites in the direct LFT compression and injection molding process as well as in combination with LGF concentrates on the injection molding process. The product is available in natural color. Applications: BJ100HP has been developed especially for applications like: front end carriers, under body shieldings, door module carriers, dashboard carriers, and battery supports.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.904 g/ccISO 1183
Melt Flow 90 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 25.0 MPa50mm/min; ISO 527-2
Elongation at Break 10 %ISO 527-2
Tensile Modulus 1300 MPa1mm/min; ISO 527-2
Charpy Impact Unnotched 41.0 kJ/m²
@Temperature -20.0 °C
ISO 179/1eU
 75.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CISO 3146
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 220 - 270 °Cmass temperature
Mold Temperature 30.0 - 60.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman POLYAXIS® PD2000 Polypropylene
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer
A. Schulman POLYFORT™ PP 2801 Homopolymer Polypropylene
A. Schulman PP 828-01 Polypropylene Molding Grade Impact Polypropylene
Borealis BJ380MO Polypropylene Copolymer

PBOREA327 / 108587

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.