MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Borealis BJ380MO Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: BJ380MO is a very high melt flow heterophasic copolymer with high/medium impact strength and stiffness. This grade is designed for high-speed injection molding and contains nucleating and antistatic additives. This polymer is a CR (controlled rheology) grade with narrow molecular weight distribution giving low warpage. Components molded from this grade have good demolding properties and combine good stiffness, gloss and antistatic properties with good low-temperature impact strength. Applications: thin wall containers, square containers, closures, lids.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.906 g/cc0.0327 lb/in³ISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm0.010 - 0.020 in/in
Melt Flow 80 g/10 min
@Load 2.16 kg,
Temperature 230 °C
80 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8989ISO 2309-2
Tensile Strength, Yield 25.0 MPa3630 psi50mm/min; ISO 527-2
Elongation at Yield 5.0 %5.0 %50mm/min; ISO 527-2
Tensile Modulus 1.30 GPa189 ksi1mm/min; ISO 527-2
Charpy Impact, Notched  0.400 J/cm²
@Temperature -20.0 °C
1.90 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Puncture Energy  10.0 J
@Temperature -20.0 °C
7.38 ft-lb
@Temperature -4.00 °F
ISO 6603-2
 12.0 J
@Temperature 0.000 °C
8.85 ft-lb
@Temperature 32.0 °F
ISO 6603-2
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C199 °FISO 75-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 260 °C410 - 500 °F
Mold Temperature 20.0 - 50.0 °C68.0 - 122 °F
Hold Pressure 20.0 - 50.0 MPa2900 - 7250 psi
 
Descriptive Properties
Injection Velocityhighest possible

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis BJ356MO Polypropylene Copolymer
Borealis BJ100HP Polypropylene Copolymer
Borealis BJ360MO Polypropylene Copolymer
Shinkong Synthetic Fibers Shinite® D201 PBT
Borealis BH345MO Polypropylene Copolymer

PBOREA330 / 108590

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.