MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Fibre Glast 3101 3K, 2x2 Twill Weave Prepreg Carbon Fiber Fabric
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: Prepreg fabrics are pre-impregnated with an epoxy resin system. As a result, nearly perfect resin content and maximum, repeatable strength properties are attainable. When properly fabricated, parts made with Fibre Glast prepregs will have a clear shine and be free of air bubbles. Although prepreg material addresses many of the nagging challenges of composite fabrication, the user’s fabrication techniques will directly affect the finished properties and cosmetics. Fibre Glast prepregs are easy to handle and are able to be stored, shipped and handled at room temperatures. These prepregs have a shelf life of 12 months when the maximum storage temperature does not exceed 75°F and 6 months when it does not exceed 90°F.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 3.9 %Neat Resin
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 169 °FNeat Resin; After 24 hr water boil
 270 °FNeat Resin; G" on DMA Curve
 
Processing PropertiesOriginal ValueComments
Processing Temperature 270 °F
@Time 14400 sec
Target Cure Temp
 290 °F
@Time 7200 sec
Target Cure Temp
 310 °F
@Time 3600 sec
Target Cure Temp
 
Descriptive Properties
Weave Pattern2x2 twill
Weight (oz/sq yd)6.8
Yarn Description, Fill3K Multifilament Cont. Tow
Yarn Description, Warp3K Multifilament Cont. Tow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Fibre Glast 1069 3K, 2x2 Twill Weave Carbon Fiber Fabric
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, 3K High Strength Carbon
Park Aerospace Nelcote® E-763 Epoxy Prepreg, 3K 2x2 Twill Carbon Reinforced
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Unidirectional Carbon Prepreg M46J Fibre
E-Glass Fiber, Generic

PFIBRE113 / 104550

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.