MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Ertalon® 4.6 PA 4.6, extruded (ISO Data)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46); Nylon 46, Unreinforced

Material Notes: Compared with conventional nylons, Ertalon 4.6 features a better retention of stiffness and creep resistance over a wide range of temperatures as well as superior heat ageing resistance. Therefore, applications for Ertalon 4.6 are situated in the “higher temperature area” (80 – 150 °C) where stiffness, creep resistance, heat ageing resistance, fatigue strength and wear resistance of PA 6, PA 66, POM and PET fall short.

  • High mechanical strength, stiffness, hardness and toughness
  • Good fatigue resistance
  • High mechanical damping ability
  • Good sliding properties
  • Excellent wear resistance
  • Good electrical insulating properties
  • Good resistance to high energy radiation (gamma- and X-rays)
  • Good machinability

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccISO 1183-1
Moisture Absorption at Equilibrium 2.8 %50% RH
Water Absorption at Saturation 9.5 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 92ISO 2039-2
Hardness, Shore D 80
Ball Indentation Hardness 165 MPaISO 2039-1
Tensile Strength, Yield 105 MPaISO 527-1/-2
Elongation at Break 25 %ISO 527-1/-2
Elongation at Yield 18 %ISO 527-1/-2
Tensile Modulus 3400 MPaISO 527-1/-2
Flexural Strength 138 MPa
Flexural Modulus 3230 MPa
Compressive Strength 31.0 MPa
@Strain 1 %
ISO 604
 60.0 MPa
@Strain 2 %
ISO 604
 102 MPa
@Strain 5.0 %
ISO 604
K Factor (ISO) 18 µm/km
Charpy Impact Unnotched NBISO 179-1/1eU
Charpy Impact, Notched 8.00 kJ/m²ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.40 - 0.60
Limiting Pressure Velocity 0.100 MPa-m/secat 1 m/s unlubricated
 0.160 MPa-m/secat 0.1 m/s unlubricated
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.0e+14 ohm-cmIEC 60093
Surface Resistivity per Square >= 1.0e+13 ohmIEC 60093
Dielectric Constant 3.8
@Frequency >=100000 Hz
IEC 60250
Dielectric Strength 25.0 kV/mm
Dissipation Factor 0.0090
@Frequency 100000 Hz
IEC 60250
Comparative Tracking Index 400 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°C
@Temperature 23.0 - 100 °C
Thermal Conductivity 0.300 W/m-K
Melting Point 290 °CDSC, 10°C/min.; ISO 11357-1/-3
Maximum Service Temperature, Air 130 °CContinuous; 20,000 h
 150 °CContinuous; 5,000 h
Deflection Temperature at 1.8 MPa (264 psi) 160 °CISO 75-1/-2
Flammability, UL94 HB
Oxygen Index 24 %ISO 4589-1/-2
 
Compliance PropertiesOriginal ValueComments
3A-Dairy No
European Food 1935/2004 No
FDA No
USP Class VI No
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Unacceptable
Acids, Weak Limited
Alcohols Limited
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Limited
Chlorinated Solvents Limited
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Ertalon® 66 GF30 PA 66, 30% glass filled, extruded (ISO Data)
Mitsubishi Chemical Advanced Materials Ertalon® 6 SA PA 6, extruded (ISO Data)
Akro-Plastic Akromid® A3 (2414) PA 6.6 Dry
Hippe PA 46 Nylon 46
Mitsubishi Chemical Advanced Materials Nylatron® 101 PA66 Extruded, Unfilled, Type 66 Natural and Black (ASTM Product Data Sheet)

P1SMU838 / 130659

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.