MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Mitsubishi Chemical Advanced Materials Ertalon® 4.6 PA 4.6, extruded (ISO Data)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46); Nylon 46, Unreinforced

Material Notes: Compared with conventional nylons, Ertalon 4.6 features a better retention of stiffness and creep resistance over a wide range of temperatures as well as superior heat ageing resistance. Therefore, applications for Ertalon 4.6 are situated in the “higher temperature area” (80 – 150 °C) where stiffness, creep resistance, heat ageing resistance, fatigue strength and wear resistance of PA 6, PA 66, POM and PET fall short.

  • High mechanical strength, stiffness, hardness and toughness
  • Good fatigue resistance
  • High mechanical damping ability
  • Good sliding properties
  • Excellent wear resistance
  • Good electrical insulating properties
  • Good resistance to high energy radiation (gamma- and X-rays)
  • Good machinability

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Density 1.19 g/cc0.0430 lb/in³ISO 1183-1
Moisture Absorption at Equilibrium 2.8 %2.8 %50% RH
Water Absorption at Saturation 7.00 %7.00 %ASTM D570 (17)
 9.5 %9.5 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9292ISO 2039-2
 92.092.0ASTM D785
Hardness, Shore D 8080
 80.080.0ISO 868
Ball Indentation Hardness 165 MPa23900 psiISO 2039-1
Tensile Strength 105 MPa15200 psiISO 527-1/-2 (7)
Tensile Strength, Yield 105 MPa15200 psiISO 527-1/-2
Elongation at Break 25 %25 %ISO 527-1/-2
Elongation at Yield 18 %18 %ISO 527-1/-2
 18.0 %18.0 %ISO 527-1/-2 (7)
Tensile Modulus 3.40 GPa493 ksiISO 527-1/-2
Flexural Strength 138 MPa20000 psi
 138 MPa20000 psiISO 178 (12)
Flexural Modulus 3.23 GPa468 ksi
Compressive Yield Strength  31.0 MPa
@Strain 1.00 %
4500 psi
@Strain 1.00 %
ISO 604 (10)
 60.0 MPa
@Strain 2.00 %
8700 psi
@Strain 2.00 %
ISO 604 (10)
 102 MPa
@Strain 5.00 %
14800 psi
@Strain 5.00 %
ISO 604 (10)
Compressive Strength  31.0 MPa
@Strain 1 %
4500 psi
@Strain 1 %
ISO 604
 60.0 MPa
@Strain 2 %
8700 psi
@Strain 2 %
ISO 604
 102 MPa
@Strain 5.0 %
14800 psi
@Strain 5.0 %
ISO 604
K Factor (ISO) 18 µm/km18 µm/km
Charpy Impact Unnotched NBNBISO 179-1/1eU
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²ISO 179-1/1eA
 0.800 J/cm²3.81 ft-lb/in²ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.40 - 0.600.40 - 0.60
Limiting Pressure Velocity 0.100 MPa-m/sec2860 psi-ft/minat 1 m/s unlubricated
 0.160 MPa-m/sec4570 psi-ft/minat 0.1 m/s unlubricated
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.0e+14 ohm-cm>= 1.0e+14 ohm-cmIEC 60093
Surface Resistivity per Square >= 1.0e+13 ohm>= 1.0e+13 ohmIEC 60093
 1.00e+14 ohm1.00e+14 ohmANSI/ESD STM 11.11
Dielectric Constant 3.8
@Frequency >=100000 Hz
3.8
@Frequency >=100000 Hz
IEC 60250
Dielectric Strength 25.0 kV/mm635 kV/in
 25.0 kV/mm635 kV/inIEC 60243-1 (15)
Dissipation Factor 0.0090
@Frequency 100000 Hz
0.0090
@Frequency 100000 Hz
IEC 60250
Comparative Tracking Index 400 V400 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°FASTM E-831 (TMA)
 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 140 °F
 90.0 µm/m-°C
@Temperature 23.0 - 100 °C
50.0 µin/in-°F
@Temperature 73.4 - 212 °F
 90.0 µm/m-°C
@Temperature 23.0 - 100 °C
50.0 µin/in-°F
@Temperature 73.4 - 212 °F
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°F
 0.300 W/m-K2.08 BTU-in/hr-ft²-°F
 0.303 W/m-K2.10 BTU-in/hr-ft²-°F
Melting Point 290 °C554 °FDSC, 10°C/min.; ISO 11357-1/-3
 290 °C554 °FASTM D3418
Maximum Service Temperature, Air 129 °C265 °FContinuous Use Temperature in Air after 20000 hr
 130 °C266 °FContinuous; 20,000 h
 150 °C302 °FContinuous; 5,000 h
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FISO 75-1/-2
 160 °C320 °FASTM D648
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Flammability, UL94 HBHB
Oxygen Index 24 %24 %ISO 4589-1/-2
 
Compliance PropertiesMetricEnglishComments
3A-Dairy NoNo
European Food 1935/2004 NoNo
FDA NoNo
USP Class VI NoNo
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) UnacceptableUnacceptable
 LimitedLimited
Acids, Weak LimitedLimited
 LimitedLimited
Alcohols LimitedLimited
 AcceptableAcceptable
Alkalies, Strong (pH 11-14) UnacceptableUnacceptable
 AcceptableAcceptable
Alkalies, Weak LimitedLimited
 AcceptableAcceptable
Chlorinated Solvents LimitedLimited
 AcceptableAcceptable
Continuous Sunlight LimitedLimited
 LimitedLimited
Hot Water / Steam LimitedLimited
 LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
 AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
 AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
 AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 AcceptableAcceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Ertalon® 66 GF30 PA 66, 30% glass filled, extruded (ISO Data)
Mitsubishi Chemical Advanced Materials Ertalon® 6 SA PA 6, extruded (ISO Data)
Akro-Plastic Akromid® A3 (2414) PA 6.6 Dry
Hippe PA 46 Nylon 46
Mitsubishi Chemical Advanced Materials Nylatron® 101 PA66 Extruded, Unfilled, Type 66 Natural and Black (ASTM Product Data Sheet)

P1SMU838 / 130659

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.