MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
3M 9443NP Double Coated Tapes with Adhesive 700 Series
Categories: Polymer; Adhesive

Material Notes: 3M™ Double Coated Tapes with 3M™ Adhesive 700 Series feature a high tack synthetic rubber adhesive which provides excellent quick stick or initial adhesion and bonds together a wide variety of materials such as metals, papers, paints and most plastics. These tapes have a film carrier, which can add dimensional stability for aid in removal and also provides easier handling during slitting and die-cutting.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 2.00 milFaceside Adhesive
 2.00 milCarrier
 2.00 milBackside Adhesive
 4.00 milLiner Caliper
 6.00 milTape Caliper
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 5.3125 plito Polypropylene, 90°, 2 mil Al foil, 72 hr RT; ASTM D3330
 5.5625 plito Polyester, 90°, 2 mil Al foil, 72 hr RT; ASTM D3330
 5.625 plito Stainless Steel, 90°, 2 mil Al foil, 15 min RT; ASTM D3330
 6.0625 plito Stainless Steel, 90°, 2 mil Al foil, 72 hr RT; ASTM D3330
 6.3125 plito Polycarbonate, 90°, 2 mil Al foil, 72 hr RT; ASTM D3330
 7.875 plito Stainless Steel, 90°, 2 mil Al foil, 72 hr at 70°C; ASTM D3330
 12.875 plito Stainless Steel, 90°, 2 mil Al foil, 72 hr RT; ASTM D3330
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 49.0 °CLong term
 70.0 °CShort term
 
Processing PropertiesOriginal ValueComments
Shelf Life 18.0 Month
 
Descriptive Properties
AppearanceClear
LinerGreen plaid, 60# Densified Kraft

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM33256 / 168003

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.