MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M 9443NP Double Coated Tapes with Adhesive 700 Series
Categories: Polymer; Adhesive

Material Notes: 3M™ Double Coated Tapes with 3M™ Adhesive 700 Series feature a high tack synthetic rubber adhesive which provides excellent quick stick or initial adhesion and bonds together a wide variety of materials such as metals, papers, paints and most plastics. These tapes have a film carrier, which can add dimensional stability for aid in removal and also provides easier handling during slitting and die-cutting.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 milFaceside Adhesive
 50.8 microns2.00 milCarrier
 50.8 microns2.00 milBackside Adhesive
 102 microns4.00 milLiner Caliper
 152 microns6.00 milTape Caliper
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.93128 kN/m5.3125 plito Polypropylene, 90°, 2 mil Al foil, 72 hr RT; ASTM D3330
 0.97511 kN/m5.5625 plito Polyester, 90°, 2 mil Al foil, 72 hr RT; ASTM D3330
 0.9861 kN/m5.625 plito Stainless Steel, 90°, 2 mil Al foil, 15 min RT; ASTM D3330
 1.0628 kN/m6.0625 plito Stainless Steel, 90°, 2 mil Al foil, 72 hr RT; ASTM D3330
 1.1066 kN/m6.3125 plito Polycarbonate, 90°, 2 mil Al foil, 72 hr RT; ASTM D3330
 1.380 kN/m7.875 plito Stainless Steel, 90°, 2 mil Al foil, 72 hr at 70°C; ASTM D3330
 2.2570 kN/m12.875 plito Stainless Steel, 90°, 2 mil Al foil, 72 hr RT; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 49.0 °C120 °FLong term
 70.0 °C158 °FShort term
 
Processing PropertiesMetricEnglishComments
Shelf Life 18.0 Month18.0 Month
 
Descriptive Properties
AppearanceClear
LinerGreen plaid, 60# Densified Kraft

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM33256 / 168003

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.