MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Elantas Conap FR-1046 / EA-02 Conapoxy® Resin / Conacure® Hardener
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes:
Epoxy Potting and Encapsulating Systems for Electronic Applications
High technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive and related industries.

Cytec (Conap) FR-1046 / EA-02 Conapoxy® Resin / Conacure® Hardener
A filled, non-abrasive, low viscosity, low shrinkage, low exotherm system with excellent resistance to thermal shock and very good electrical insulation properties. Low cost.
  • Mix Ratio, Resin/Hardener (by weight): 100/5.5
Cure Type: Room Temperature

Information provided by Cytec, subsequently acquired by Elantas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 6800 cP
@Temperature 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 88
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 6.00e+15 ohm-cm
Dielectric Constant 5.5
@Frequency 1000 Hz
Dielectric Strength 375 V/mil
Dissipation Factor 0.0050
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 130 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hour
@Temperature 25.0 °C
Pot Life 30.0 min
@Temperature 25.0 °C
100 grams

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay Thornel® T-300 1K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Solvay Thornel® T-40 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Solvay FM® 377S Adhesive Film, psf 0.06 (293 gsm)
Solvay Thornel® T-605/50X 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Solvay VTA® 260 Adhesive Film

PCYTEC32 / 29264

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.