MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for PETG Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); PETG Copolyester

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.18 - 1.37 g/ccAverage value: 1.27 g/cc Grade Count:75
Water Absorption 0.120 - 0.200 %Average value: 0.146 % Grade Count:5
Moisture Absorption at Equilibrium 0.200 - 0.300 %Average value: 0.250 % Grade Count:5
Viscosity Test 70.0 - 86.0 cm³/gAverage value: 77.0 cm³/g Grade Count:6
Linear Mold Shrinkage 0.00140 - 0.00700 cm/cmAverage value: 0.00359 cm/cm Grade Count:38
Melt Flow 1.20 - 39.0 g/10 minAverage value: 15.3 g/10 min Grade Count:12
ASTM Color 1.00 - 68.0Average value: 33.0 Grade Count:4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 104 - 121Average value: 110 Grade Count:31
Tensile Strength, Ultimate 20.0 - 100 MPaAverage value: 44.8 MPa Grade Count:62
Tensile Strength, Yield 28.3 - 101 MPaAverage value: 51.4 MPa Grade Count:48
Elongation at Break 3.20 - 360 %Average value: 123 % Grade Count:64
Elongation at Yield 2.70 - 575 %Average value: 31.0 % Grade Count:35
Modulus of Elasticity 1.10 - 20.3 GPaAverage value: 3.03 GPa Grade Count:39
Flexural Yield Strength 39.2 - 88.9 MPaAverage value: 70.5 MPa Grade Count:44
Flexural Modulus 1.17 - 2.76 GPaAverage value: 1.97 GPa Grade Count:59
Izod Impact, Notched 0.267 - 5340 J/cmAverage value: 3.81 J/cm Grade Count:37
 0.290 - 0.520 J/cm
@Temperature -40.0 - -30.0 °C
Average value: 0.407 J/cm Grade Count:6
Izod Impact, Unnotched 0.497 J/cm - NBAverage value: 6.94 J/cm Grade Count:11
 0.277628 J/cm - NB
@Temperature -40.0 - -40.0 °C
Average value: 0.278 J/cm Grade Count:3
Izod Impact, Notched (ISO) 4.00 kJ/m² - NBAverage value: 7.41 kJ/m² Grade Count:14
 4.40 - 4.40 kJ/m²
@Temperature -40.0 - -30.0 °C
Average value: 4.40 kJ/m² Grade Count:4
Izod Impact, Unnotched (ISO) NB - NB
@Temperature -30.0 - -30.0 °C
Grade Count:1
Charpy Impact Unnotched 1000 J/cm² - NBGrade Count:10
 999.9 J/cm² - NB
@Temperature -30.0 - 0.000 °C
Grade Count:4
Charpy Impact, Notched 0.153 - 1.00 J/cm²Average value: 0.668 J/cm² Grade Count:17
 0.310 - 0.500 J/cm²
@Temperature -30.0 - 0.000 °C
Average value: 0.443 J/cm² Grade Count:4
Falling Dart Impact 542.328 - 542.328 J
@Temperature -40.0 - -40.0 °C
Average value: 542 J Grade Count:1
Puncture Energy 44.0 - 44.0 J
@Temperature -40.0 - -40.0 °C
Average value: 44.0 J Grade Count:1
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 10.0 - 1.00e+16 ohm-cmAverage value: 1.72e+15 ohm-cm Grade Count:24
Surface Resistance 1000 - 1.00e+16 ohmAverage value: 9.38e+14 ohm Grade Count:20
Static Decay 0.0100 - 2.00 secAverage value: 0.785 sec Grade Count:11
Dielectric Constant 2.40 - 3.46Average value: 2.64 Grade Count:10
Dielectric Strength 10.7 - 30.0 kV/mmAverage value: 17.9 kV/mm Grade Count:10
Dissipation Factor 0.00500 - 0.0230Average value: 0.0160 Grade Count:7
 
Thermal PropertiesOriginal ValueComments
CTE, linear 43.0 - 94.0 µm/m-°CAverage value: 64.6 µm/m-°C Grade Count:17
Specific Heat Capacity 1.10 - 1.30 J/g-°CAverage value: 1.20 J/g-°C Grade Count:4
Thermal Conductivity 0.162 - 0.225 W/m-KAverage value: 0.197 W/m-K Grade Count:9
Maximum Service Temperature, Air 60.0 - 78.6 °CAverage value: 69.6 °C Grade Count:6
Deflection Temperature at 0.46 MPa (66 psi) 60.0 - 109 °CAverage value: 73.4 °C Grade Count:41
Deflection Temperature at 1.8 MPa (264 psi) 55.0 - 92.0 °CAverage value: 65.8 °C Grade Count:49
Vicat Softening Point 70.0 - 85.0 °CAverage value: 78.0 °C Grade Count:19
Glass Transition Temp, Tg 79.0 - 85.0 °CAverage value: 80.9 °C Grade Count:12
Decomposition Temperature 70.0 - 280 °CAverage value: 228 °C Grade Count:4
Flammability, UL94 HB - V-2Grade Count:11
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.57Average value: 1.57 Grade Count:6
Haze 0.200 - 1.10 %Average value: 0.897 % Grade Count:29
Gloss 90.0 - 171 %Average value: 148 % Grade Count:4
Transmission, Visible 74.0 - 95.0 %Average value: 87.5 % Grade Count:32
UV Transmittance 53.0 - 90.0 %Average value: 77.4 % Grade Count:10
 
Processing PropertiesOriginal ValueComments
Processing Temperature 45.0 - 260 °CAverage value: 193 °C Grade Count:15
Die Temperature 195 - 293 °CAverage value: 244 °C Grade Count:10
Melt Temperature 160 - 293 °CAverage value: 231 °C Grade Count:27
Mold Temperature 10.0 - 70.0 °CAverage value: 28.6 °C Grade Count:13
Drying Temperature 50.0 - 102 °CAverage value: 68.7 °C Grade Count:24
Moisture Content 0.00400 - 0.300 %Average value: 0.0354 % Grade Count:16
Dew Point -40.0 - -33.9 °CAverage value: -36.1 °C Grade Count:11
Injection Pressure 5.50 - 103 MPaAverage value: 70.0 MPa Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polylactic Acid (PLA) Biopolymer
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
Eastman Eastar GN071 Natural PETG Copolyester
Overview of materials for Polycarbonate, Extruded

O3380 / 78207

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.