MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hanwha Azdel Plus R401-B01 40% Continuous Random Fiber Mat / PP Resin Matrix
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: AZDEL® R401-B01 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a polypropylene resin matrix. This composite material features high flow properties and a very homogeneous fiber distribution. This material is typically used for standard semi-structural applications where high stiffness and impact are desired.

Mechanical properties and mold shrinkage measured on flat plaques.

Information provided by Azdel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccLaminate; ASTM D792
 1.21 g/ccMolded; ASTM D792
Filler Content 40 %By weight (ashing); Internal
Thickness 3700 micronsSheet; Internal
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cmMeasured on flat plaques; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 108 MPaISO 527
Elongation at Break 2.5 %ISO 527
Tensile Modulus 6.16 GPaISO 527
Flexural Strength 160 MPaISO 178
Flexural Modulus 6.15 GPaISO 178
Poissons Ratio 0.361ISO 527
Izod Impact, Notched 810 J/m
@Thickness 4.00 mm,
Temperature 23.0 °C
ISO 180
Impact 384
@Thickness 4.00 mm
Multi-axial in kg, at max. load; ASTM D3763
Impact Test 15.0 J
@Thickness 4.00 mm
Multi-axial, at max. load; ASTM D3763
 28.0 J
@Thickness 4.00 mm
Multi-axial, at failure; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear 43.0 µm/m-°C
@Temperature -40.0 - 120 °C
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 154 °CASTM D648
Flame Spread 2.8 mm/minFMVSS302
 
Descriptive Properties
ColorBlackInternal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hanwha Azdel Plus R300-B01 30% Continuous Random Fiber Mat / PP Resin Matrix
Hanwha Azdel AZMET® CM32350 35% continuous random fiber mat / PET resin matrix
Hanwha Azdel AZMET® CM20350 35% continuous random fiber mat / PBT resin matrix
Hanwha Azdel Plus R451-B02 45% Continuous Random Fiber Mat / PP Resin Matrix
Hanwha Azdel Plus C467-B01 45% Chopped Fiber Mat / PP Resin Matrix (Mineral filled)

PZZGEAZ67 / 40616

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.