AZDEL® CM20350 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a Polybutylene Terephthalate (PBT) resin matrix. This composite material features high flow properties and a generally homogeneous fiber distribution. This material is typically used for standard semi-structural applications where high stiffness and impact are desired. Mechanical properties and mold shrinkage measured on flat plaques. Information provided by Azdel. |