MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ATI Allegheny Ludlum Stainless Steel Ohmaloy® 40 Resistance Alloy
Categories: Metal; Electronic/Magnetic Alloy; Ferrous Metal

Material Notes: Ohmaloy 40 alloy is a moderately magnetic, ductile stainless steel having extremely high electrical resistivity. In addition to imparting high electrical resistivity, the aluminum content in these iron-13% chromium-aluminum resistance alloys also provides oxidation resistance. This alloy are capable of resisting oxidation for continuous duty at temperature up to 982 degrees Celsius, and is satisfactory for intermittent heating in temperatures form 982 to 1038 degrees Celsius. This alloy is used in many applications requiring dissipation of electrical energy. Some examples are grid resistors for mine locomotives, crane starters and, the largest application, braking resistors for railroad diesel locomotives. This alloy is used where the application demands heavy-duty resistors with a small volume-to-volume ratio. They can also be used in applications where resistance heating is required.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.41 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 88Typical
Tensile Strength, Ultimate 600 MPaTypical
Tensile Strength, Yield 448 MPaTypical
Elongation at Break 23 %typical in 2"
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000116 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.3 µm/m-°C
@Temperature 20.0 - 100 °C
 12.2 µm/m-°C
@Temperature 20.0 - 500 °C
 14.2 µm/m-°C
@Temperature 20.0 - 1000 °C
Thermal Conductivity 14.5 W/m-K
@Temperature 50.0 °C
Maximum Service Temperature, Air 982 °C
 1038 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 3.95 %
Carbon, C 0.025 %
Chromium, Cr 13 %
Iron, Fe 82 %as balance
Manganese, Mn 0.35 %
Silicon, Si 0.30 %
Titanium, Ti 0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AK Steel 13-4 SR® Ferritic Stainless Steel
ATI Allegheny Ludlum ALFA-I™ Stainless Steel Type 406
Resistalloy International Resistalloy 3718 Nickel Chromium Electrical Resistance Alloy
Resistalloy International Fecralloy™ Electrical Resistance Steel
Resistalloy International Fecralloy™ 145 Electrical Resistance Steel

NLO40 / 18030

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.