MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
General Plastics LAST-A-FOAM® FR-10118 Polyurethane Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes:

Information provided by General Plastics Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.288 g/ccASTM D1622
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 416 psiParallel to Rise; ASTM D1623
 450 psiPerpendicular to Rise; ASTM D1623
Flexural Strength 810 psiRise Parallel to Test Span; ASTM D790
 820 psiRise Parallel to Beam Thick.; ASTM D790
Flexural Modulus 38142 psiRise Parallel to Test Span; ASTM D790
 39256 psiRise Parallel to Beam Thick.; ASTM D790
Compressive Strength 480 psi
@Temperature 177 °C
Parallel to Rise; ASTM D1621
 650 psi
@Temperature 177 °C
Perpendicular to Rise; ASTM D1621
 870 psi
@Temperature 121 °C
Parallel to Rise; ASTM D1621
 900 psi
@Temperature 121 °C
Perpendicular to Rise; ASTM D1621
 1210 psi
@Temperature 23.9 °C
Parallel to Rise; ASTM D1621
 1245 psi
@Temperature 23.9 °C
Perpendicular to Rise; ASTM D1621
Compressive Modulus 13575 psi
@Temperature 177 °C
Parallel to Rise; ASTM D1621
 16884 psi
@Temperature 177 °C
Perpendicular to Rise; ASTM D1621
 20137 psi
@Temperature 121 °C
Parallel to Rise; ASTM D1621
 20761 psi
@Temperature 121 °C
Perpendicular to Rise; ASTM D1621
 25774 psi
@Temperature 23.9 °C
Parallel to Rise; ASTM D1621
 25971 psi
@Temperature 23.9 °C
Perpendicular to Rise; ASTM D1621
Poissons Ratio 0.30
 
Thermal PropertiesOriginal ValueComments
CTE, linear 21.0 µin/in-°F
@Temperature -28.9 - 71.1 °C
GP Method
Thermal Conductivity 0.0470 BTU-in/hr-ft²-°FASTM C518
 
Descriptive Properties
Tumbling Friability (%)3.720 mins at 60 rpm, ASTM C421

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
General Plastics LAST-A-FOAM® FR-10120 Polyurethane Foam
Unifrax Excelfrax® 200 VIP Vacuum Insulation Panel
General Plastics LAST-A-FOAM® FR-10115 Foam
DIAB Rigid Foam IPN 20-649 Type 1

PGENR061 / 186847

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.