MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

General Plastics LAST-A-FOAM® FR-10118 Polyurethane Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes:

Information provided by General Plastics Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.288 g/cc0.0104 lb/in³ASTM D1622
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 2.87 MPa416 psiParallel to Rise; ASTM D1623
 3.10 MPa450 psiPerpendicular to Rise; ASTM D1623
Flexural Strength 5.58 MPa810 psiRise Parallel to Test Span; ASTM D790
 5.65 MPa820 psiRise Parallel to Beam Thick.; ASTM D790
Flexural Modulus 0.26298 GPa38.142 ksiRise Parallel to Test Span; ASTM D790
 0.27066 GPa39.256 ksiRise Parallel to Beam Thick.; ASTM D790
Compressive Strength  3.31 MPa
@Temperature 177 °C
480 psi
@Temperature 350 °F
Parallel to Rise; ASTM D1621
 4.48 MPa
@Temperature 177 °C
650 psi
@Temperature 350 °F
Perpendicular to Rise; ASTM D1621
 6.00 MPa
@Temperature 121 °C
870 psi
@Temperature 250 °F
Parallel to Rise; ASTM D1621
 6.21 MPa
@Temperature 121 °C
900 psi
@Temperature 250 °F
Perpendicular to Rise; ASTM D1621
 8.34 MPa
@Temperature 23.9 °C
1210 psi
@Temperature 75.0 °F
Parallel to Rise; ASTM D1621
 8.584 MPa
@Temperature 23.9 °C
1245 psi
@Temperature 75.0 °F
Perpendicular to Rise; ASTM D1621
Compressive Modulus  0.093596 GPa
@Temperature 177 °C
13.575 ksi
@Temperature 350 °F
Parallel to Rise; ASTM D1621
 0.11641 GPa
@Temperature 177 °C
16.884 ksi
@Temperature 350 °F
Perpendicular to Rise; ASTM D1621
 0.13884 GPa
@Temperature 121 °C
20.137 ksi
@Temperature 250 °F
Parallel to Rise; ASTM D1621
 0.14314 GPa
@Temperature 121 °C
20.761 ksi
@Temperature 250 °F
Perpendicular to Rise; ASTM D1621
 0.17771 GPa
@Temperature 23.9 °C
25.774 ksi
@Temperature 75.0 °F
Parallel to Rise; ASTM D1621
 0.17906 GPa
@Temperature 23.9 °C
25.971 ksi
@Temperature 75.0 °F
Perpendicular to Rise; ASTM D1621
Poissons Ratio 0.300.30
 
Thermal PropertiesMetricEnglishComments
CTE, linear 37.8 µm/m-°C
@Temperature -28.9 - 71.1 °C
21.0 µin/in-°F
@Temperature -20.0 - 160 °F
GP Method
Thermal Conductivity 0.00677 W/m-K0.0470 BTU-in/hr-ft²-°FASTM C518
 
Descriptive Properties
Tumbling Friability (%)3.720 mins at 60 rpm, ASTM C421

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
General Plastics LAST-A-FOAM® FR-10120 Polyurethane Foam
Unifrax Excelfrax® 200 VIP Vacuum Insulation Panel
General Plastics LAST-A-FOAM® FR-10115 Foam
DIAB Rigid Foam IPN 20-649 Type 1

PGENR061 / 186847

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.