MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
317LN High-Nitrogen Austenitic Stainless Steel, Annealed Plate, Sheet, Strip, UNS S31753
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes:

Information provided by Industeel and the references(s).

Key Words: ASTM A 167
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 95
Tensile Strength 550 MPa
Tensile Strength, Yield 240 MPa
Elongation at Break 40 %
Modulus of Elasticity 200 GPa
@Temperature 20.0 - 100 °C
Poissons Ratio 0.299Calculated
Shear Modulus 77.0 GPa
@Temperature 20.0 - 100 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000800 ohm-cm
@Temperature 20.0 - 100 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.0 µm/m-°C
@Temperature 20.0 - 100 °C
 16.5 µm/m-°C
@Temperature 20.0 - 200 °C
 17.0 µm/m-°C
@Temperature 20.0 - 300 °C
 18.0 µm/m-°C
@Temperature 20.0 - 500 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 20.0 - 100 °C
Thermal Conductivity 14.0 W/m-K
@Temperature 20.0 - 100 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.030 %
Chromium, Cr 18.2 %
Iron, Fe 65.43 - 65.46 %As remainder
Molybdenum, Mo 3.2 %
Nickel, Ni 13 %
Nitrogen, N 0.14 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carlson 904L Austenitic Stainless Steel
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 900 (Age-Hardened 482°C/1hr/AC)
AK Steel 316 Austenitic Stainless steel
AK Steel 316L Austenitic Stainless steel
ATI Allvac® REX 734™ UNS S31675 Specialty Steel

MQ317LN / 172154

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.