MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Melinex® RFL1 Polyester Film, 600 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: MELINEX® RFL1 is a highly reflective, white polyester film.

Typical Applications: Typical applications include reflectors in display boards, internally illuminated billboards, labels, backlights, and luminaries.

Approvals: UL Recognition - Product has been registered with Underwriters Laboratories

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ASTM D1505
Brightness 110 %110 %Whiteness; ASTM E313-79
Thickness 152 microns6.00 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 80 %80 %ASTM D882A
Film Elongation at Break, TD 65 %65 %ASTM D882A
Film Tensile Strength at Break, MD 79.3 MPa11500 psiASTM D882A
Film Tensile Strength at Break, TD 86.2 MPa12500 psiASTM D882A
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 1.7 %
@Temperature 150 °C,
Time 1800 sec
1.7 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 1.2 %
@Temperature 150 °C,
Time 1800 sec
1.2 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Optical Density 1.31.3Densitometer with visual/ortho filter
Gloss 60 %60 %60°, Macbeth TD904 Optical; ASTM D2457-08
Transmission, Visible 2.5 %2.5 %TLT; ASTM D1003-11

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Melinex® AG2 Polyester Film
DuPont Teijin Films Melinex® AF Polyester Film
DuPont Teijin Films Melinex® 966 Polyester Film, 700 Gauge
DuPont Teijin Films Melinex® FRP Polyester Film, 92 Gauge
DuPont Teijin Films Melinex® D316 Polyester Film, 200 Gauge

PDTZ9220 / 139548

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.