MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Melinex® AF Polyester Film
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Melinex® AF is a clear polyester film coated both sides with an anti-fog coating.

Typical Applications: Typical applications include face shields, masks, visors, and other industrial uses.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 150 %150 %ASTM D882A
Film Elongation at Break, TD 100 %100 %ASTM D882A
Film Tensile Strength at Break, MD 152 MPa22000 psiASTM D882A
Film Tensile Strength at Break, TD 165 MPa24000 psiASTM D882A
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 2.5 %
@Temperature 190 °C,
Time 300 sec
2.5 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.0 %
@Temperature 190 °C,
Time 300 sec
1.0 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Haze 1.5 %1.5 %ASTM D1003
Transmission, Visible 89 %
@Thickness 0.102 - 0.165 mm
89 %
@Thickness 0.00400 - 0.00650 in
TLT; ASTM D1003
 
Descriptive Properties
Yield (nominal)3099 in2/lb650 Gauge
 5035 in2/lb400 Gauge

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Melinex® 694 Polyester Film
DuPont Teijin Films Melinex® AG2 Polyester Film
DuPont Teijin Films Melinex® 966 Polyester Film, 700 Gauge
DuPont Teijin Films Melinex® 965 Polyester Film, 500 Gauge
DuPont Teijin Films Melinex® 943 Polyester Film

PDTZ9204 / 139540

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.