MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials PEARLCOAT® 127K Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: PEARLCOAT® 127K is a polyester based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low-temperature flexibility and medium softening point. PEARLCOAT® 127K is used in melt coatings on textile substrates for conveyor belts, belting, among other end uses, obtained by extrusion, calendering or sintering (in this last case the product is previously ground, so as to be in powder form).

All information provided by Merquinsa

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 92ASTM D2240
Tensile Strength, Yield 4360 psiASTM D412
Elongation at Break 430 %ASTM D412
50% Modulus 8.00 MPa
@Strain 50 %
ISO 527-2/5A/500
100% Modulus 1.162 ksi
@Strain 100 %
ASTM D412
300% Modulus 2.325 ksi
@Strain 300 %
ASTM D412
Tear Strength 93.0 kN/mUnnicked; ISO 34-1B
Abrasion 30Resistance (mm³); ISO 4649-A
 
Processing PropertiesOriginal ValueComments
Drying Temperature 90.0 °C
Dry Time 3.00 hour
Dew Point <= -30.0 °C
 
Descriptive Properties
Roll 1160°C
Roll 2170°C
Rubber Roll 3not heated

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Austin Novel Materials Texalan® 598A Polyether-based TPU
Austin Novel Materials Texalan® 698A Polyester and Polyether based TPU
Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer
Taiwan PU Corporation TPU-EH95 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU
Lubrizol Estane® ETE 75DT3 Thermoplastic Polyurethane, Easy-to-Extrude

PMES75 / 88452

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.