MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

3M Scotchcast™ 262 Electrical Epoxy Powder Resin
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: 3M Scotchcast Electrical Resin 262 is a widely used, well-known general purpose epoxy powder resin. A one-part, red pigmented, rapid heat-curing product, it is designed to provide a continuous, tough moisture and chemical resistant dielectric coating to a variety of substrates.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³cured; ASTM D794
 
Mechanical PropertiesMetricEnglishComments
Gardner Impact 11.3 J8.33 ft-lb12-15 mil coating 1/8" sandblasted steel panel Gardner 5/8: Radius Impact Tester
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 39.4 kV/mm1000 kV/in12 to 15 mil coating; ASTM D149
 
Processing PropertiesMetricEnglishComments
Cure Time  0.500 min
@Temperature 232 °C
0.00833 hour
@Temperature 450 °F
 1.00 min
@Temperature 204 °C
0.0167 hour
@Temperature 399 °F
 20.0 min
@Temperature 177 °C
0.333 hour
@Temperature 351 °F
 40.0 min
@Temperature 149 °C
0.667 hour
@Temperature 300 °F
Gel Time 0.200 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min
@Temperature 193 °C
0.200 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min
@Temperature 379 °F
hot plate
Shelf Life 24.0 Month
@Temperature <=27.0 °C
24.0 Month
@Temperature <=80.6 °F
 
Descriptive Properties
AppearanceRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotchcast™ 2131 Flame-Retardant Compound
3M Scotchcast™ 5388 Electrical Epoxy Powder Resin
3M Scotchcast™ 2104 Electrical Insulating Resin

PMM35361 / 170108

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.