MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Scotchcast™ 2131 Flame-Retardant Compound
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: 3M Scotchcast Flame-Retardant Compound 2131 is a two-part polyurethane resin designed to replace the cable jacket when splicing or repairing mine and portable cables. It formulation makes it particularly suited to withstand the rugged conditions under which mine and portable cables must operate. Flame-Retardant Compound 2131 is also used as the insulating material for cable splices operating at up to 1000 volts and designed for 90°C continuous use/130°C overload. When used in accordance with the appropriate kit configuration, Compound 2131 meets Part 7, Title 30 CFR and carries the following MSHA approvals.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.217 g/cc0.04397 lb/in³
Moisture Absorption 4.90 %4.90 %ASTM D471
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8282ASTM D2240
Tensile Strength at Break 7.16 MPa1040 psiASTM D412
Elongation at Break 339 %339 %ASTM D412
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  5.22
@Frequency 60.0 Hz,
Temperature 23.0 °C
5.22
@Frequency 60.0 Hz,
Temperature 73.4 °F
ASTM D150
 6.33
@Frequency 60.0 Hz,
Temperature 60.0 °C
6.33
@Frequency 60.0 Hz,
Temperature 140 °F
ASTM D150
 6.56
@Frequency 60.0 Hz,
Temperature 90.0 °C
6.56
@Frequency 60.0 Hz,
Temperature 194 °F
ASTM D150
Dielectric Strength 13.5 kV/mm343 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -75.0 °C-103 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  960 - 1440 min
@Temperature 21.0 °C
16.0 - 24.0 hour
@Temperature 69.8 °F
De-Mold Time: 1.5-2 hrs
 1440 - 1800 min
@Temperature 10.0 °C
24.0 - 30.0 hour
@Temperature 50.0 °F
De-Mold Time: 3.5-4 hrs
 >= 2160 min
@Temperature 0.000 °C
>= 36.0 hour
@Temperature 32.0 °F
De-Mold Time: 6-8 hrs
Gel Time 17.0 min17.0 min3M Method TM-87
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Miracll E180F Halogen-Free Flame Retardant TPU
Clariant OMAN698583 Thermoplastic Polyurethane, Halogen Free, Flame Retardant
BASF Elastollan® 1185 A FHF TPUR Flame Retardant Halogen Free
AlphaGary Garathane™ 9006 Polyurethane based compound
3M Scotchcast™ 5388 Electrical Epoxy Powder Resin

PMM35236 / 169983

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.