MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Everest™ 200 Latex Modified Acrylic Emulsion  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Applications:EVEREST 200 is based on a unique modified acrylic technology, that was developed to address the growing interest in carpet backing technologies with sustainable attributes. This high solids emulsion offers properties that are not available in styrene butadiene latexes used in the carpet industry today. Whether the application is for commercial broadloom or carpet tile, compounds made with EVEREST 200 are stable to a wide range of Post Industrial and Post Consumer recycled fillers, which allow carpet manufacturers to maximize the amount of recycled content in their products. For example, in a typical 200 load formulation using recycled filler, 30-35% of the weight of the carpet would be based on recycled content. Carpet backed with EVEREST 200 yields physical properties similar to current technologies even in the presence of plasticizers, making this product ideal for many carpet tile pre-coats. Whether looking to improve the environmental footprint of commercial broadloom product or modular tile system, EVEREST 200 meets the needs. As with all carpet backing products from Dow, EVEREST Technology is designed to pass all CRI Green Label Plus VOC standards.

Benefits:

  • High Solids
  • Excellent recycle filler acceptance
  • Excellent Plasticizer Migration Resistance
  • Excellent heat age stability

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/cc
Solids Content 55 %
Particle Size 2.8 µm
pH 6.8
Brookfield Viscosity 225 cP#3 @ 50 rpm
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 8.80 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow C133-02 Polypropylene Impact Copolymer Resin
Dow CYCLOTENE™ 3022-57 Bisbenzocyclobutene (BCB) Electronic Resin
Dow ELITE™ 5100G Enhanced Polyethylene Resin
Dow INSPIRE™ 112 Performance Polymer
Dow SiLK™ I300 560 Semiconductor Dielectric Resin

PDWST111 / 142320

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.