MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow ELITE™ 5100G Enhanced Polyethylene Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: ELITE™ 5100G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers excellent impact strength, good tensile and puncture properties for thick and thin gauge industrial and consumer blown film applications. This resin exhibits higher hot tack strengths than LLDPE, making it ideal for automated packaging applications.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D792
Thickness 50.8 microns2.00 mil
Melt Flow 0.85 g/10 min0.85 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 11.80 MPa1712 psiASTM D882
Film Tensile Strength at Yield, TD 12.5 MPa1810 psiASTM D882
Film Elongation at Break, MD 595 %595 %ASTM D882
Film Elongation at Break, TD 652 %652 %ASTM D882
Secant Modulus, MD 0.2216 GPa32.14 ksi2% Secant; ASTM D882
Secant Modulus, TD 0.2575 GPa37.35 ksi2% Secant; ASTM D882
Impact 2424[lbf]; Puncture Resistance Force; Dow Method
 249249[ft-lbf/in3]; Puncture Resistance; Dow Method
Puncture Energy 9.04 J6.67 ft-lbDow Method
Elmendorf Tear Strength MD 707 g707 gASTM D1922
Elmendorf Tear Strength TD 1033 g1033 gASTM D1922
Elmendorf Tear Strength, MD 13.92 g/micron353.5 g/milASTM D1922
Elmendorf Tear Strength, TD 20.33 g/micron516.5 g/milASTM D1922
Dart Drop Test 780 g1.72 lbMethod B; ASTM D1709
Film Tensile Strength at Break, MD 57.27 MPa8307 psiASTM D882
Film Tensile Strength at Break, TD 53.47 MPa7755 psiASTM D882
Heat Seal Strength Initiation Temperature 106 °C223 °F2 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
 
Thermal PropertiesMetricEnglishComments
Melting Point 124 °C255 °FDow Method (DSC)
Vicat Softening Point 105 °C221 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 10 %10 %ASTM D1003
Gloss 67 %67 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow DOWLEX™ 2045G Linear Low Density Polyethylene
Borealis Borstar® FB2230 LLDPE for Film
Dow ELITE™ 5500G Enhanced Polyethylene Resin
Dow DOWLEX™ 2045.11G Linear Low Density Polyethylene
Dow ELITE™ 5400G Enhanced Polyethylene Resin

PDOW1322 / 30540

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.