System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Celanese SO.F.TER Sofprene® P Ski Boots 0C0280D40
Categories:
Polymer
;
Thermoplastic
;
Elastomer, TPE
;
Thermoplastic Olefinic Elastomer (TPO)
Material Notes:
Ski Boots, Elastomer-modified polyolefin compound, highly resistant to low temperatures
Information provided by SO.F.TER. Spa
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.950
g/cc
0.0343
lb/in³
ASTM D 792
Linear Mold Shrinkage
0.0080
-
0.013
cm/cm
0.0080
-
0.013
in/in
Melt Flow
35
g/10 min
35
g/10 min
ASTM 1238
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
40
40
ASTM D 2240
Tensile Strength
13.0
MPa
1890
psi
ASTM D412
Elongation at Break
700 %
700 %
ASTM D412
Flexural Modulus
0.280
GPa
40.6
ksi
ASTM D790
Izod Impact Resistance
NB
NB
ASTM D256
Tear Strength
66.0
kN/m
377
pli
ASTM D624 C
Compression Set
7.5 %
7.5 %
ASTM D395
Processing Properties
Metric
English
Comments
Processing Temperature
180
-
200
°C
356
-
392
°F
Descriptive Properties
Features
available in all colors
Surface Appearance
matte covered
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 25A, Non-Black Sulfur Cure
Wacker ELASTOSIL® R plus 4105/40 Solid Silicone Rubber-Batch Grade
Wacker Elastosil® R plus 4001/30 Silicone Rubber
Teknor Apex Sarlink® TPE EE-2340DN XRD Thermoplastic Elastomer
Teknor Apex Monprene® CP-3090D XRD Thermoplastic Elastomer
PSOFS653 / 162117
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.