Physical Properties | Metric | English | Comments |
---|
Density | 7.87 g/cc | 0.284 lb/in³ |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Brinell | 121 @Diameter 50.8 - 76.2 mm | 121 @Diameter 2.00 - 3.00 in |
| 131 @Diameter 31.8 - 50.8 mm | 131 @Diameter 1.25 - 2.00 in |
| 143 @Diameter 22.2 - 31.8 mm | 143 @Diameter 0.875 - 1.25 in |
| 149 @Diameter 15.9 - 22.2 mm | 149 @Diameter 0.625 - 0.875 in |
Hardness, Knoop | 140 @Diameter 50.8 - 76.2 mm | 140 @Diameter 2.00 - 3.00 in |
| 150 @Diameter 31.8 - 50.8 mm | 150 @Diameter 1.25 - 2.00 in |
| 163 @Diameter 22.2 - 31.8 mm | 163 @Diameter 0.875 - 1.25 in |
| 169 @Diameter 15.9 - 22.2 mm | 169 @Diameter 0.625 - 0.875 in |
Hardness, Rockwell B | 68 @Diameter 50.8 - 76.2 mm | 68 @Diameter 2.00 - 3.00 in |
| 73 @Diameter 31.8 - 50.8 mm | 73 @Diameter 1.25 - 2.00 in |
| 78 @Diameter 22.2 - 31.8 mm | 78 @Diameter 0.875 - 1.25 in |
| 80 @Diameter 15.9 - 22.2 mm | 80 @Diameter 0.625 - 0.875 in |
Hardness, Vickers | 126 @Diameter 50.8 - 76.2 mm | 126 @Diameter 2.00 - 3.00 in |
| 136 @Diameter 31.8 - 50.8 mm | 136 @Diameter 1.25 - 2.00 in |
| 149 @Diameter 22.2 - 31.8 mm | 149 @Diameter 0.875 - 1.25 in |
| 155 @Diameter 15.9 - 22.2 mm | 155 @Diameter 0.625 - 0.875 in |
Tensile Strength, Ultimate | 415 MPa @Diameter 50.8 - 76.2 mm | 60200 psi @Diameter 2.00 - 3.00 in |
| 450 MPa @Diameter 31.8 - 50.8 mm | 65300 psi @Diameter 1.25 - 2.00 in |
| 485 MPa @Diameter 22.2 - 31.8 mm | 70300 psi @Diameter 0.875 - 1.25 in |
| 515 MPa @Diameter 15.9 - 22.2 mm | 74700 psi @Diameter 0.625 - 0.875 in |
Tensile Strength, Yield | 345 MPa @Diameter 50.8 - 76.2 mm | 50000 psi @Diameter 2.00 - 3.00 in |
| 380 MPa @Diameter 31.8 - 50.8 mm | 55100 psi @Diameter 1.25 - 2.00 in |
| 415 MPa @Diameter 22.2 - 31.8 mm | 60200 psi @Diameter 0.875 - 1.25 in |
| 450 MPa @Diameter 15.9 - 22.2 mm | 65300 psi @Diameter 0.625 - 0.875 in |
Elongation at Break | 12 % @Diameter 50.8 - 76.2 mm | 12 % @Diameter 2.00 - 3.00 in |
| 13 % @Diameter 31.8 - 50.8 mm | 13 % @Diameter 1.25 - 2.00 in |
| 15 % @Diameter 15.9 - 22.2 mm | 15 % @Diameter 0.625 - 0.875 in |
| 15 % @Diameter 22.2 - 31.8 mm | 15 % @Diameter 0.875 - 1.25 in |
Reduction of Area | 30 % @Diameter 50.8 - 76.2 mm | 30 % @Diameter 2.00 - 3.00 in |
| 35 % @Diameter 31.8 - 50.8 mm | 35 % @Diameter 1.25 - 2.00 in |
| 40 % @Diameter 15.9 - 22.2 mm | 40 % @Diameter 0.625 - 0.875 in |
| 40 % @Diameter 22.2 - 31.8 mm | 40 % @Diameter 0.875 - 1.25 in |
Modulus of Elasticity | 200 GPa | 29000 ksi |
Bulk Modulus | 160 GPa | 23200 ksi |
Poissons Ratio | 0.29 | 0.29 |
Shear Modulus | 80.0 GPa | 11600 ksi |
Izod Impact | 108 J | 79.7 ft-lb |
|
Electrical Properties | Metric | English | Comments |
---|
Electrical Resistivity | 0.0000174 ohm-cm | 0.0000174 ohm-cm |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 °C | 6.39 µin/in-°F @Temperature 68.0 °F |
| 12.2 µm/m-°C @Temperature 0.000 - 300 °C | 6.78 µin/in-°F @Temperature 32.0 - 572 °F |
| 13.9 µm/m-°C @Temperature 0.000 - 500 °C | 7.72 µin/in-°F @Temperature 32.0 - 932 °F |
Specific Heat Capacity | 0.472 J/g-°C | 0.113 BTU/lb-°F |
Thermal Conductivity | 51.9 W/m-K | 360 BTU-in/hr-ft²-°F |
|
Component Elements Properties | Metric | English | Comments |
---|
Carbon, C | 0.14 - 0.20 % | 0.14 - 0.20 % |
Iron, Fe | 98.03 - 98.48 % | 98.03 - 98.48 % |
Manganese, Mn | 1.3 - 1.6 % | 1.3 - 1.6 % |
Phosphorus, P | <= 0.040 % | <= 0.040 % |
Sulfur, S | 0.080 - 0.13 % | 0.080 - 0.13 % |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.