MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Viton® GB Process Aid
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: Description: Viton® FreeFlow™ GB is a blended fluoropolymer processing additive powder designed for improved performance in polyethylene resins. The additive contains 50% fluoropolymer powder and 50% granular polyethylene.

Advantages:

  • Viton® FreeFlow™ GB has significantly more effectiveness than conventional fluoroelastomers in polyethylene formulations. It has been specially designed for reduced interactions with other polyethylene additives. Viton® FreeFlow™ GB will give improved processing at lower fluoropolymer concentration levels than conventional fluoroelastomer.
  • Processing improvements in all types of polyolefins
  • Ease of feeding when high blend ratios are required
  • Ease of handling
  • Easily dispersed due to fine particle starting point
  • Uniformity of low ratio blends is improved over pellet blends

Information provided by manufacturer.

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 - 1.29 g/cc
 
Descriptive Properties
Active Ingredients48-52% in 1 Ml LLDPE
AppearancePale white to light amber, uniform free-flowing powder
Package Stability4 yr
Packaging25 kg containers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
TIMCAL ENSACO™ 250G Conductive Carbon Black Compounds
Saint-Gobain Norton® OmniFlex™ Fluoroelastomer High Performance Seal Material (Milky White)
Saint-Gobain Fluran® F-5500-A Fluoroelastomer Tubing
Mid-Mountain Materials ARMATEX® SF7 Silicone Rubber Coated Glass Fabric
ExxonMobil Santoprene® 8291-85TL Thermoplastic Elastomer

PDVDA69 / 34038

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.