MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plastcom SLOVAMID® 6 GF 10 T 20 TS 002 Polyamide 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced

Material Notes: PA 6 for injection molding reinforced with 10% glass fiber and 20% talc, heat stabilized. Good anisotropy of the manufacturing shrinkage.

Application for flat products in disc form - low warp age after cooling off and for thick-walled products. Delivered in natural and in the full RAL color scale.

Information Provided by Plastcom spol. s r.o.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³STN EN ISO 1183-1
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/inSTN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inSTN EN ISO 294-4
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
10 g/10 min
@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 100 MPa14500 psiSTN EN ISO 527-2
Elongation at Break 3.0 %3.0 %STN EN ISO 527-2
Tensile Modulus 6.30 GPa914 ksiSTN EN ISO 527-2
Flexural Strength 155 MPa22500 psiSTN EN ISO 178
Flexural Modulus 4.50 GPa653 ksiSTN EN ISO 178
Charpy Impact Unnotched  3.50 J/cm²
@Temperature -20.0 °C
16.7 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
Charpy Impact, Notched  0.200 J/cm²
@Temperature -20.0 °C
0.952 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 0.300 J/cm²
@Temperature 23.0 °C
1.43 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmSTN 34 6460
Surface Resistance 1.00e+14 ohm1.00e+14 ohmSTN 34 6460
Dielectric Strength 25.0 kV/mm635 kV/inSTN EN 60243-2
Comparative Tracking Index 450 V450 VA; STN EN 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °FDSC; STN EN ISO 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FSTN EN ISO 75-2 (A)
Vicat Softening Point 210 °C410 °FB; STN EN ISO 306
Flammability, UL94 HBHB
Glow Wire Flammability Index 650 °C
@Thickness 3.00 mm
1200 °F
@Thickness 0.118 in
STN EN 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 280 °C482 - 536 °F
Mold Temperature 70.0 - 90.0 °C158 - 194 °F
Drying Temperature 80.0 °C
@Time 14400 sec
176 °F
@Time 4.00 hour
Moisture Content 0.10 %0.10 %STN EN ISO 3344
Injection Pressure 60.0 - 150 MPa8700 - 21800 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPLACN904 / 282496

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.