PA 6 for injection molding reinforced with 10% glass fiber and 20% talc, heat stabilized. Good anisotropy of the manufacturing shrinkage. Application for flat products in disc form - low warp age after cooling off and for thick-walled products. Delivered in natural and in the full RAL color scale. Information Provided by Plastcom spol. s r.o. |