MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Crastin® SK642FR NC010 Polybutylene Terephthalate (PBT)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled

Material Notes: 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate

Crastin SK642FR is a 15% glass fibre reinforced flame retardant polybutylene terephthalate for injection moulding.It has a UL94 V-0 rating @ 1.5mm.

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Key Words: PBT-GF15FR(17)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/cc
 1.58 g/ccISO 1183
Water Absorption 0.33 %
@Thickness 2.00 mm
Sim. to ISO 62
Moisture Absorption 0.140 %
@Thickness 2.00 mm
Sim. to ISO 62
Viscosity 102700 cP
@Shear Rate 5000 1/s,
Temperature 260 °C
ISO 11403-1 -2
 122300 cP
@Shear Rate 5000 1/s,
Temperature 250 °C
ISO 11403-1 -2
 147800 cP
@Shear Rate 5000 1/s,
Temperature 240 °C
ISO 11403-1 -2
 310520 cP
@Shear Rate 500 1/s,
Temperature 260 °C
ISO 11403-1 -2
 375900 cP
@Shear Rate 500 1/s,
Temperature 250 °C
ISO 11403-1 -2
 460190 cP
@Shear Rate 500 1/s,
Temperature 240 °C
ISO 11403-1 -2
Linear Mold Shrinkage, Flow 0.0070 cm/cmISO 294-4 2577
 0.0080 cm/cmannealed; ISO 294-4
Linear Mold Shrinkage, Transverse 0.012 cm/cmISO 294-4 2577
 0.015 cm/cmannealed; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 100 MPaISO 527-1/-2
Elongation at Break 3.4 %ISO 527-1/-2
Tensile Modulus 7200 MPaISO 527-1/-2
Flexural Strength 155 MPaISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
Izod Impact, Unnotched (ISO) 33.0 kJ/m²ISO 180/1U
 32.0 kJ/m²
@Temperature -30.0 °C
ISO 180/1U
Charpy Impact Unnotched 53.0 kJ/m²ISO 179/1eU
 44.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²ISO 179/1eA
 7.10 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
Tensile Creep Modulus, 1 hour 6000 MPa
@Time 3600 sec
ISO 899-1
Tensile Creep Modulus, 1000 hours 4800 MPa
@Time 3.60e+6 sec
ISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohmIEC 60093
Dielectric Constant 3.5
@Frequency 1e+6 Hz
IEC 60250
 3.7
@Frequency 100 Hz
IEC 60250
Dielectric Strength 28.0 kV/mmIEC 60243-1
Dissipation Factor 0.0030
@Frequency 100 Hz
IEC 60250
 0.017
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 250 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 50.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°CISO 11359-1/-2
Specific Heat Capacity 1.74 J/g-°C
Thermal Conductivity 0.270 W/m-Kof melt
Melting Point 225 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 218 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 203 °CISO 75-1/-2
Vicat Softening Point 207 °C50°C/h 50N; ISO 306
Flammability, UL94 V-0
@Thickness 1.50 mm
IEC 60695-11-10
 V-0
@Thickness 0.800 mm
IEC 60695-11-10
Oxygen Index 31 %ISO 4589-1/-2
 
Descriptive Properties
Delivery formPellets
Part Marking Code>PBT-GF15FR(17)<ISO 11469
ProcessingInjection Molding
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPBT-GF15FR(17)
UL recognitionUL

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Crastin® S650FR NC010 PBT-FR(17)
Celanese Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT)
Celanese Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT)
Celanese Crastin® ST830FRUV NC010 PBT-HIFR(17)
Chang Chun Plastic PBT4115 Fire Retardant & 15% Glass Fiber Enforced Grade PBT

PZDSY5083 / 160910

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.